| Category | Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Molded |
| Manufacturer | |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | 3M Dyneon™ TFM™ 1705 Modified PTFE Powder
(discontinued **).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 2.16 g/cc | 0.0780 lb/in³ | ASTM D4894 |
| Apparent Bulk Density | 0.420 g/cc | 0.0152 lb/in³ | ASTM D4894 |
| Particle Size | 25 µm | 25 µm | ASTM D4894 |
| Deformation | 2.0 % <br>@Pressure 15.00 MPa |
2.0 % <br>@Pressure 2175 psi |
ASTM D621 |
| 4.0 % <br>@Time 86400 sec,<br> Pressure 15.00 MPa |
4.0 % <br>@Time 24.0 hour,<br> Pressure 2175 psi |
ASTM D621 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore D | 62 | 62 | Initial; ASTM D2240 |
| 58 <br>@Time 15.0 sec |
58 <br>@Time 0.00417 hour |
ASTM D2240 | |
| Tensile Strength at Break | 333 MPa | 48300 psi | ASTM D4894 |
| Elongation at Break | 450 % | 450 % | ASTM D4894 |
| Tensile Modulus | 0.650 GPa | 94.3 ksi | ASTM D638 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 59.0 µm/m-°C <br>@Temperature 30.0 - 100 °C |
32.8 µin/in-°F <br>@Temperature 86.0 - 212 °F |
ASTM E831 |
| 77.0 µm/m-°C <br>@Temperature 100 - 200 °C |
42.8 µin/in-°F <br>@Temperature 212 - 392 °F |
ASTM E831 | |
| 93.0 µm/m-°C <br>@Temperature 200 - 300 °C |
51.7 µin/in-°F <br>@Temperature 392 - 572 °F |
ASTM E831 | |
| Thermal Conductivity | 0.220 W/m-K <br>@Temperature 100 °C |
1.53 BTU-in/hr-ft²-°F <br>@Temperature 212 °F |
ASTM E831 |
| 0.230 W/m-K <br>@Temperature 250 °C |
1.60 BTU-in/hr-ft²-°F <br>@Temperature 482 °F |
ASTM E831 | |
| Shrinkage | 5.8 % | 5.8 % | ASTM D4894 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Strength | 3.70 kV/mm | 94.0 kV/in | ASTM D 149 |