Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.420 g/cc | 0.0152 lb/in³ | Geon® STP 1169; Internal Method |
PolyOne Geon™ Specialty Suspension Atlas E 46 Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® Atlas E 46 is high molecular weight homopolymer specialty suspension resin intended for use in high strength extruded parts. It improves the physical performance of end application for instan.. |
|||
Apparent Bulk Density | 0.420 g/cc | 0.0152 lb/in³ | ASTM D4894 |
3M Dyneon™ TFM™ 1705 Modified PTFE Powder
(discontinued **) Type II, gr. 1 PTFE. Dyneon™ TFM™ 1705 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-generat.. |
|||
Apparent Bulk Density | 0.420 g/cc | 0.0152 lb/in³ | TRM-37 |
Tipco Tipcolite® TMS 211 Phenolic Compound, Cotton, Filler & Wood Flour, having Medium Flow & High Strength Medium Flow Phenolic Compound, Reinforced with Cotton, Filler & Wood FlourApplications: Industrial & AutomotivesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr.. |
|||
Apparent Bulk Density | 0.420 g/cc | 0.0152 lb/in³ | TRM-37 |
Tipco Tipcolite® TMS 311 Phenolic Compound, Cotton, Filler & Wood Flour, having Medium Flow & High Strength Medium Flow Phenolic Compound, Reinforced with Cotton, Filler & Wood FlourApplications: Industrial & AutomotivesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industr.. |
|||
Apparent Bulk Density | 0.420 g/cc | 0.0152 lb/in³ | ASTM D4894 |
3M Dyneon™ TFM™ 1700 Modified PTFE Powder Type III, gr. 1 PTFE. Dyneon™ TFM™ 1700 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-genera.. |