Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 333 MPa | 48300 psi | ASTM D4894 |
3M Dyneon™ TFM™ 1705 Modified PTFE Powder
(discontinued **) Type II, gr. 1 PTFE. Dyneon™ TFM™ 1705 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-generat.. |