Material Notes:
LD5000A is a low-density polyethylene with good mechanical properties, good ESCR, and excellent sealing characteristics. It does not contain additives. It is used in general purpose blow molded articles and injection blow molding.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ASTM-D1505
Melt Flow 1.4 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.4 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.0 MPa
2180 psi
ASTM-D638
Tensile Strength, Yield 12.0 MPa
1740 psi
ASTM-D638
Thermal Properties Metric English Comments
Vicat Softening Point 94.0 °C

@Load 1.02 kg
201 °F

@Load 2.25 lb
ASTM-D1525