Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 0.230 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.230 W/m-K

@Temperature 195 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 383 °F
Pyrotek ISOMAG® 70 Structural Insulation
Isomag® 70 is magnesia silicate based formulation provides insulating properties similar to calcium silicate with good strength and dimensional stability up to 1000°C. ApplicationsTorpedo cars La..
Thermal Conductivity 0.230 W/m-K

@Temperature 1650 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 3000 °F
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation
Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo..
Thermal Conductivity 0.230 W/m-K

@Temperature 100 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1530
3M Dyneon™ TR 1105 PTFE  (discontinued **)
Ideal for thin wall ram extrusion productsReduces cold flow and melt viscosityLower permeabilityLower porosityWeldableExcellent product smoothnessIncreased machine outputInformation provided by Dyne..
Thermal Conductivity 0.230 - 0.310 W/m-K

@Temperature 600 °C
1.60 - 2.15 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 125 R Refractory Insulating Castable
Description: Golite 125 R has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products. Also availa..
Thermal Conductivity 0.230 - 0.330 W/m-K

@Temperature 100 °C
1.60 - 2.29 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 135 RL C Refractory Insulating Castable
Description: Golite 135 RL C is a coarse low iron light weight castable and combines a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast ..
Thermal Conductivity 0.230 W/m-K

@Temperature 200 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; ASTM C-182
Skamol Group VIP 12 Vermiculite Insulating Slab
SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr..
Thermal Conductivity 0.230 W/m-K

@Temperature 816 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 1500 °F
8 pcf
Thermal Ceramics Cerablanket Blanket
Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on ave..
Thermal Conductivity 0.230 W/m-K

@Temperature 816 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 1500 °F
8 pcf
Thermal Ceramics Cerachem Blanket
Cerachem Blanket is a 2600°F (1427°C) maximum temperature rated refractory blanket formed from a unique, patented, spun alumina-silica-zirconia fiber. It is specially designed for applications whe..
Thermal Conductivity 0.230 W/m-K

@Temperature 816 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 1500 °F
8 pcf
Thermal Ceramics Kaowool S Blanket
Kaowool S Blanket is produced from high quality spun fibers. It is available in a wide variety of densities and sizes, and offers a highly cost effective alternative to Cerablanket with its 2300°F ..
Thermal Conductivity 0.230 W/m-K

@Temperature 1200 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics AB Alumina Blanket
Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with ..
Thermal Conductivity 0.230 W/m-K

@Temperature 1350 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 2460 °F
Parallel to thickness; ASTM C177-76
Zircar Ceramics AL-30 Alumina Insulation
AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C..
Thermal Conductivity 0.230 W/m-K

@Temperature 1350 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 2460 °F
parallel to thickness; ASTM C177-76
Zircar Ceramics AL-30AAH Alumina Insulation
AL-30AAH was developed for use in copper vapor lasers where the ultimate in low mass alumina purity is required.Information provided by Zircar Ceramics.
Thermal Conductivity 0.230 W/m-K

@Temperature 1200 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Parallel to thickness; ASTM C177-76
Zircar Ceramics MB Alumina Blanket
Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with ..
Thermal Conductivity 0.230 W/m-K

@Temperature 1650 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 3000 °F
Zircar Zirconia ZYC Zirconia Cylinders Insulation
Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing ..
Thermal Conductivity 0.230 W/m-K

@Temperature 1650 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 3000 °F
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation
Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo..
Thermal Conductivity 0.230 W/m-K

@Temperature 1100 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation
Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo..
Thermal Conductivity 0.230 W/m-K

@Temperature 1200 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 2190 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics Alumina Mat
A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between..
Thermal Conductivity 0.230 W/m-K

@Temperature 816 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C182
BNZ Materials BNZ-23 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.230 W/m-K

@Temperature 1093 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 1999 °F
ASTM C182
BNZ Materials BNZ-24 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.230 W/m-K

@Temperature 260 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 500 °F
ASTM C182
BNZ Materials BNZ-26 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.230 W/m-K

@Temperature 600 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C182
BNZ Materials BNZP-23B Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.230 W/m-K

@Temperature 600 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C182
BNZ Materials BNZP-25L Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.230 W/m-K

@Temperature 600 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C182
BNZ Materials BNZP-26A Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.230 W/m-K

@Temperature 200 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 392 °F
ASTM C182
BNZ Materials BNZP-26HS Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.230 W/m-K

@Temperature 200 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 392 °F
ASTM C182
BNZ Materials Color B Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.230 W/m-K

@Temperature 260 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 500 °F
ASTM C182
BNZ Materials PA 23 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.230 W/m-K

@Temperature 250 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 482 °F
ASTM D1530
3M Dyneon™ TFM™ 1700 Modified PTFE Powder
Type III, gr. 1 PTFE. Dyneon™ TFM™ 1700 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-genera..
Thermal Conductivity 0.230 W/m-K

@Temperature 1650 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 3000 °F
Zircar Zirconia ZYC Zirconia Cylinders Insulation
Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing ..
Thermal Conductivity 0.230 W/m-K

@Temperature 1350 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 2460 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics AL-30AA Alumina Insulation
AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C..
Thermal Conductivity 0.230 W/m-K

@Temperature 1000 °C
1.60 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Parallel to Thickness
Zircar Ceramics ECO-27B Alumina-Silica Insulation
This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-27 offers exceptional strength and durability. Information provided by Zircar Cer..
Copyright © lookpolymers.com All Rights Reserved