Williams Advanced Alloys WS186 Solder

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Williams Advanced Alloys
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Williams Advanced Alloys WS186 Solder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Physical Properties Metric English Comments
Density 8.17 g/cc
0.295 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 53.8 MPa
7800 psi
Thermal Properties Metric English Comments
CTE, linear 27.0 µm/m-°C

@Temperature 20.0 °C
15.0 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 53.0 W/m-K
368 BTU-in/hr-ft²-°F
Melting Point 183 - 186 °C
361 - 367 °F
Solidus 183 °C
361 °F
Liquidus 186 °C
367 °F
Component Elements Properties Metric English Comments
Lead, Pb 30 %
30 %
Tin, Sn 70 %
70 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00001376 ohm-cm
0.00001376 ohm-cm