Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 25 µm | 25 µm | D<sub>50</sub>; ISO 13320-1 |
Victrex® PEEK 150XF Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, fine powder for compression moulding, easy flow, FDA food contact compliant, .. |
|||
Particle Size | 25 µm | 25 µm | ASTM D4894 |
3M Dyneon™ CCX1029 PTFE, 10% Carbon Fiber Filled
(discontinued **) Type I, non-free-flowing.Typical Applications: Finished or semi-finished parts: sheets, rods, tubes, billets for skiving of films or machining into complex shapes.Information provided by the Dyneon .. |
|||
Particle Size | 25 µm | 25 µm | ASTM D4894 |
3M Dyneon™ CC174-N PTFE, 15% Fiberglass/Moly Filled
(discontinued **) Product Form: Gray, non-pelletized powder. Applications include bearings, rider rings, and packings.Data provided by Dyneon. |
|||
Particle Size | 25 µm | 25 µm | median |
3M Dyneon™ PFA 6503 A EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **) Dyneon PFA 6503 A EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick .. |
|||
Particle Size | 25 µm | 25 µm | median |
3M Dyneon™ PFA 6503 C EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **) Dyneon PFA 6503 C EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick .. |
|||
Particle Size | 25 µm | 25 µm | ASTM D4894 |
3M Dyneon™ CC191-HE Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of high elongation 23% carbon / 2% graphite blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
Particle Size | <= 25 µm | <= 25 µm | MVG Powder |
Ferro EG 0221 Specialty Glass Glass Type: MG-Al-Si (devitrified) Typical Powder Form: MVG, SRRG Typical Application: Sintering Aid / Ceramic Ferro offers a wide range of compositions for specialty applications including sinteri.. |
|||
Particle Size | <= 25 µm | <= 25 µm | |
Ferro EG 2739 Thick Film Glass Glass Type: Pb-Zn-B Typical Powder Form: MVG Typical Application: Resistor Overglaze Ferro produces standard and custom glass products that are used in thick film compositions including resistors, .. |
|||
Particle Size | <= 25 µm | <= 25 µm | |
Ferro EG 2778 Thick Film Glass Glass Type: Si-Al-Ca Typical Powder Form: MVG Typical Application: Dielectric Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduct.. |
|||
Particle Size | <= 25 µm | <= 25 µm | |
Ferro EG 2783 Thick Film Glass Glass Type: Pb-B Typical Powder Form: MVG Typical Application: Die Attachment Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conduct.. |
|||
Particle Size | <= 25 µm | <= 25 µm | RWG Powder |
Ferro IP 760 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | <= 25 µm | <= 25 µm | RWG Powder |
Ferro IP 780 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 25 - 29 µm | 25 - 29 µm | 90% |
H.C. Starck Amperit® 281 Gas Atomized (NiAl 95-5) |
|||
Particle Size | 25 µm | 25 µm | Average Particle Size/Laser Diffraction D50 |
H.C. Starck Grade P1 Crystalline Boron Neutron shields and absorbers in nuclear reactorsThermistorsFilamentsPreparation of high-purity metal boridesMetallurgy (deoxidizing agent) |
|||
Particle Size | <= 25 µm | <= 25 µm | |
Ferro EG 0002 Glazes and Sealants Glass Type: Si-Al-Ba Typical Powder Form: VWG Typical Application: SiC Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulatin.. |
|||
Particle Size | <= 25 µm | <= 25 µm | |
Ferro IP 510 Thick Film Glass Glass Type: Pb-Si-B-Al Typical Powder Form: RWG Typical Application: General Ferro produces standard and custom glass products that are used in thick film compositions including resistors, conducto.. |
|||
Particle Size | <= 25 µm | <= 25 µm | RWG Powder |
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | <= 25 µm | <= 25 µm | RWG Powder |
Ferro IP 745 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | <= 25 µm | <= 25 µm | RWG Powder |
Ferro IP 770 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 25 µm | 25 µm | Before Conversion |
Silberline Sparkle Silvet® Premier 860-30-E1 Sparkle Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final .. |
|||
Particle Size | 25 µm | 25 µm | |
UCAR Carbon UCAR® ATJ Isostatic Molded Graphite Isostatically molded ATJ has been an industry standard for many years. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish. Grade ATJ has.. |
|||
Particle Size | 25 µm | 25 µm | |
UCAR Carbon UCAR® ATR Isostatic Molded Graphite Isostatically molded ATR is a lower density version of grade ATJ. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish.Typical Application.. |
|||
Particle Size | 25 µm | 25 µm | |
UCAR Carbon UCAR® CGW Isostatic Molded Graphite Isostatically molded grade CGW is an ATJ-based material that has been processed to higher density and strength. Grade CGW is characterized by low permeability, erosion resistance and surface hardnes.. |
|||
Particle Size | 25 µm | 25 µm | d90 |
TIMCAL TIMREX® MX25 Primary Synthetic Graphite TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro.. |
|||
Particle Size | 25 - 27 µm | 25 - 27 µm | D50 |
CIMBAR UltraMag & UltraMag ST 60-90 Magnesium Hydroxide Powder UltraMag is a naturally ground, white, high-purity Magnesium Hydroxide suitable for a wide range of applications including water treatment slurries, plastics, rubber and flame-retardant/smoke suppre.. |
|||
Particle Size | 25 µm | 25 µm | average; ASTM D4894-98a |
3M Dyneon™ TFM™ 1705 PTFE Non-free-flowing resinReduced, adjusted melt viscosityIncreased gel stabilityReduced cold flowLower porosity and permeabilityLower void contentExcellent non-stick and dielectric propertiesHigher ela.. |
|||
Particle Size | 25 µm | 25 µm | |
Asahi Glass Fluon® G163 PTFE Granular Powder Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc. |
|||
Particle Size | 25 µm | 25 µm | 10th% |
3M K25 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 25 µm | 25 µm | average; ASTM D4894-98a |
3M Dyneon™ TF 1750 PTFE Meets ASTM D4894 Type IINon-free-flowing powder gradeVery fine particle sizeGood electrical and mechanical propertiesLow molding pressureUsed in large billet moldingExcellent for production of very .. |
|||
Particle Size | 25 µm | 25 µm | Mean |
Momentive Performance Materials PolarTherm® PTX25 Boron Nitride (BN) Powder Spherical BN Agglomeration Powder. Spherical nature may improve thermal conductivity at moderate loading levels when used as a filler in polymers or lubricants, and produce less anisotropic propert.. |