Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.230 W/m-K @Temperature 195 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 383 °F |
|
Pyrotek ISOMAG® 70 Structural Insulation Isomag® 70 is magnesia silicate based formulation provides insulating properties similar to calcium silicate with good strength and dimensional stability up to 1000°C. ApplicationsTorpedo cars La.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 1650 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 3000 °F |
|
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 250 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 482 °F |
ASTM E831 |
3M Dyneon™ TFM™ 1705 Modified PTFE Powder
(discontinued **) Type II, gr. 1 PTFE. Dyneon™ TFM™ 1705 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-generat.. |
|||
Thermal Conductivity | 0.230 - 0.310 W/m-K @Temperature 600 °C |
1.60 - 2.15 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GOLITE 125 R Refractory Insulating Castable Description: Golite 125 R has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products. Also availa.. |
|||
Thermal Conductivity | 0.230 - 0.330 W/m-K @Temperature 100 °C |
1.60 - 2.29 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Gouda Vuurvast GOLITE 135 RL C Refractory Insulating Castable Description: Golite 135 RL C is a coarse low iron light weight castable and combines a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast .. |
|||
Thermal Conductivity | 0.230 - 0.330 W/m-K @Temperature 200 °C |
1.60 - 2.29 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Gouda Vuurvast GI 26 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 200 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-182 |
Skamol Group VIP 12 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 816 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 1500 °F |
8 pcf |
Thermal Ceramics Cerablanket Blanket Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on ave.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 816 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 1500 °F |
8 pcf |
Thermal Ceramics Cerachem Blanket Cerachem Blanket is a 2600°F (1427°C) maximum temperature rated refractory blanket formed from a unique, patented, spun alumina-silica-zirconia fiber. It is specially designed for applications whe.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 816 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 1500 °F |
8 pcf |
Thermal Ceramics Cerachrome Blanket Made from spun alumina-silica-chromia fiber, Cerachrome Blanket is well suited for hot face lining applications where higher temperatures are encountered, such as soaking pit covers, reheat and forg.. |
|||
Thermal Conductivity | 0.231 W/m-K @Temperature 1090 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 2000 °F |
|
Thermal Ceramics Kaowool HD Low Temperature Board Kaowool HD is a low cost high strength product recommended for tough mechanical stress areas. Also, very good for back-up behind dense refractories.Features: Excellent thermal conductivity Capabilit.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 816 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 1500 °F |
8 pcf |
Thermal Ceramics Kaowool S Blanket Kaowool S Blanket is produced from high quality spun fibers. It is available in a wide variety of densities and sizes, and offers a highly cost effective alternative to Cerablanket with its 2300°F .. |
|||
Thermal Conductivity | 0.231 - 0.245 W/m-K @Temperature 816 °C |
1.60 - 1.70 BTU-in/hr-ft²-°F @Temperature 1500 °F |
ASTM C201 |
Thermal Ceramics TC-23 Low Temperature Insulating Firebrick Thermal Ceramics was first to introduce insulating firebrick (IFB) to the industry in the 1930’s. The IFB are manufactured with a slurry casting process which creates a network of microporosity whi.. |
|||
Thermal Conductivity | 0.231 W/m-K @Temperature 260 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 500 °F |
ASTM C201 |
Thermal Ceramics TC-26 High Temperature Insulating Firebrick The bond developed is a ceramic bond that is formed by high temperature firing. This produces bricks that are very stable and strong at temperatures higher than 2600°F (1427°C). Features:High temp.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 1200 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 2190 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics AB Alumina Blanket Two varieties of quilted alumina fiber blanket that have good handleability and offer very low thermal conductivity. These resilient blankets are easily cut and applied to numerous application with .. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 1350 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 2460 °F |
parallel to thickness; ASTM C177-76 |
Zircar Ceramics AL-30AAH Alumina Insulation AL-30AAH was developed for use in copper vapor lasers where the ultimate in low mass alumina purity is required.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 1000 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 1830 °F |
Parallel to Thickness |
Zircar Ceramics ECO-27A Alumina-Silica Insulation This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-27 offers exceptional strength and durability. Information provided by Zircar Cer.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 1650 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 3000 °F |
|
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 1100 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 2010 °F |
|
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 1200 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 2190 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics Alumina Mat A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 1093 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 1999 °F |
ASTM C182 |
BNZ Materials BNZ-24 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 600 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTM C182 |
BNZ Materials BNZP-23B Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 600 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 1110 °F |
ASTM C182 |
BNZ Materials BNZP-26A Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 200 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 392 °F |
ASTM C182 |
BNZ Materials BNZP-26HS Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 260 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 500 °F |
ASTM C182 |
BNZ Materials PA 23 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 250 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 482 °F |
ASTM D1530 |
3M Dyneon™ TFM™ 1700 Modified PTFE Powder Type III, gr. 1 PTFE. Dyneon™ TFM™ 1700 PTFE is a second-generation modified polytetrafluoro-ethylene (PTFE) that maintains the exceptional chemical and heat resistance properties of first-genera.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 1650 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 3000 °F |
|
Zircar Zirconia ZYC Zirconia Cylinders Insulation Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing .. |
|||
Thermal Conductivity | 0.231 W/m-K @Temperature 816 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 1500 °F |
ASTM C201 |
Thermal Ceramics IFB 23 Tile Low Temperature Insulating Firebrick Thermal Ceramics was first to introduce insulating firebrick (IFB) to the industry in the 1930’s. The IFB are manufactured with a slurry casting process which creates a network of microporosity whi.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 1350 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 2460 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics AL-30AA Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 1000 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 1830 °F |
Parallel to Thickness |
Zircar Ceramics ECO-27B Alumina-Silica Insulation This utility grade board is produced with or without organic binder. Useful to temperatures of 1260°C (2300°F) ECO-27 offers exceptional strength and durability. Information provided by Zircar Cer.. |