Processing Properties Metric English Comments
Melt Temperature 195 - 225 °C
383 - 437 °F
SABIC 726 Series Linear Low Density Polyethylene for Blown Film
Product Description: 726 series resins are fractional index Linear Low Density Polyethylene grades suitable for blown film applications. Films produced using these resins give a relatively higher ..
Melt Temperature 200 - 225 °C
392 - 437 °F
SABIC FI0644 Bimodal High Density Polyethylene for Blown Film
Product Description: FI0644 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Melt Temperature 200 - 225 °C
392 - 437 °F
SABIC FI0750 Bimodal High Density Polyethylene for Blown Film
Product Description: FI0750 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Melt Temperature 200 - 225 °C
392 - 437 °F
SABIC FI1157 Bimodal High Density Polyethylene for Blown Film
Product Description: FI1157 is a high molecular weight high density polyethylene copolymer grade specifically designed for blown film applications. Its high molecular weight, broad molecular weigh..
Melt Temperature 190 - 225 °C
374 - 437 °F
Premix Thermoplastics PRE-ELEC® ESD 2300
PRE-ELEC ESD 2300 is a static dissipative thermoplastic compound based on PE-HD. The dissipative property is permanent and built into the polymer chain. PRE-ELEC ESD 2300 has been developed for mult..
Melt Temperature 195 - 225 °C
383 - 437 °F
NOVA Chemicals Novapol® HD-2007-H HDPE Extrusion Resin
Features: Excellent ESCR and toughness, high strength, excellent processability, very high melt strength.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provid..
Melt Temperature 195 - 225 °C
383 - 437 °F
NOVA Chemicals Novapol® HD-2100-U MDPE Extrusion Resin
Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer.
Melt Temperature 200 - 225 °C
392 - 437 °F
PTS POM-270 27.0 MFI Acetal Copolymer
Information provided by Polymer Technology and Services, LLC (PTS).
Melt Temperature 200 - 225 °C
392 - 437 °F
PTS POM-90 9.0 MFI Acetal Copolymer
Information provided by Polymer Technology and Services, LLC (PTS).
Melt Temperature 215 - 225 °C
419 - 437 °F
NOVA Chemicals Sclair® 10B Octene VLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, excellent sealability, excellent dart impact, excellent clarity.Applications: Co-extrusion.Data provided by the manufacturer.
Melt Temperature 180 - 225 °C
356 - 437 °F
NOVA Chemicals Novapol® LE-0220-A LDPE Extrusion Resin  (discontinued **)
Features: easy processing, high melt strength.Applications: wide range of profile extrusions, tape and sheet extrusion, concentrates.Data provided by the manufacturer.
Melt Temperature 180 - 225 °C
356 - 437 °F
NOVA Chemicals Novapol® LE-0520-A LDPE Extrusion Resin  (discontinued **)
Features: easy processing, good dispersion.Applications: Additive and color concentrates for film and molding.Data provided by the manufacturer.
Melt Temperature 195 - 225 °C
383 - 437 °F
NOVA Chemicals Novapol® HD-2100-A MDPE Extrusion Resin  (discontinued **)
Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer.
Melt Temperature 185 - 225 °C
365 - 437 °F
Injection Molding
LG Chemical KEYFLEX BT 1033D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Melt Temperature 185 - 225 °C
365 - 437 °F
Extrusion Molding
LG Chemical KEYFLEX BT 1033D Ester Type TPE
Description: Injection Molding, TPC-ET, General Purpose, Low ModulusApplication: Automotive Interior, Soft Touch GripsCAS: 37282-12-5Information provided by LG Chemical
Melt Temperature 200 - 225 °C
392 - 437 °F
LG Chemical Lucet® N109 Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Melt Temperature 200 - 225 °C
392 - 437 °F
LG Chemical Lucet® N127 Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Melt Temperature 180 - 225 °C
356 - 437 °F
Iran Petrochemical (PCC) LL0209AA Linear Low Density Polyethylene
LL 0209AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. It is recommended for general purpose applications.Information provided by Iran Petrochemical Commercial Co.
Melt Temperature 210 - 225 °C
410 - 437 °F
Molding
Lubrizol Pellethane® 2363-55D Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Melt Temperature 205 - 225 °C
401 - 437 °F
Covestro Desmopan® DP 9380A Polyurethane
Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilitycomplies with VDE 0282-10ApplicationCable sheathingsHosesnon-reinforcedPreprocessin..
Melt Temperature 215 - 225 °C
419 - 437 °F
E-Polymers SEPAZ® LH40 PP Homopolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Melt Temperature 220 - 225 °C
428 - 437 °F
Beijing Ranger Chem BLUESTAR® 1079 PBT
Can be used directly for spinning, and producing color concentrates. It can also be used for production after reinforcement & compounding.Information provided by Beijing Ranger Chemical Co.
Melt Temperature 220 - 225 °C
428 - 437 °F
Beijing Ranger Chem BLUESTAR® 1084 PBT
Can be used directly for spinning, and producing color concentrates. It can also be used for production after reinforcement & compounding.Information provided by Beijing Ranger Chemical Co.
Melt Temperature 220 - 225 °C
428 - 437 °F
Beijing Ranger Chem BLUESTAR® 1110 PBT
Can be used directly for spinning, or it can be used after reinforcement & compounding. It can also be used to produce cable sheath through tackificationInformation provided by Beijing Ranger Chemic..
Melt Temperature 220 - 225 °C
428 - 437 °F
Beijing Ranger Chem BLUESTAR® 1135 PBT
Can be used directly to produce cable sheathInformation provided by Beijing Ranger Chemical Co.
Melt Temperature 215 - 225 °C
419 - 437 °F
E-Polymers SEPAZ® LC40 PP Copolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Melt Temperature 220 - 225 °C
428 - 437 °F
Beijing Ranger Chem BLUESTAR® 1120 PBT
Can be used directly to produce cable sheathInformation provided by Beijing Ranger Chemical Co.
Melt Temperature 180 - 225 °C
356 - 437 °F
NOVA Chemicals Novapol® LE-0820-AM LDPE Concentrate Resin  (discontinued **)
Features: easy processing, good dispersion.Applications: Additive and color concentrates for film and molding, non-critical extrusion coating.Data provided by the manufacturer.