Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) LL0209AA Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Butene, Film
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) LL0209AA Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LL 0209AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. It is recommended for general purpose applications.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ISO 1183
Melt Flow 0.90 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.190 GPa
27.6 ksi
MD; ISO 527
0.200 GPa
29.0 ksi
TD; ISO 527
Coefficient of Friction 0.50
0.50
ASTM D1894
Elmendorf Tear Strength MD 145 g
145 g
ASTM D1922
Elmendorf Tear Strength TD 370 g
370 g
ASTM D1922
Dart Drop Test 150 g
0.331 lb
ASTM D1709
Optical Properties Metric English Comments
Haze 12 %
12 %
ASTM D1003
Gloss 50 %
50 %
ASTM D523
Processing Properties Metric English Comments
Melt Temperature 127 °C
261 °F
180 - 225 °C
356 - 437 °F