Processing Properties | Metric | English | Comments |
---|---|---|---|
Melt Temperature | 215 °C | 419 °F | |
Multibase TPSiV® 3111-60A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Hydrolysis resistant; FDA 21 CFR 177.2600 CompliantAPPLICATIONS: Solution for soft touc.. |
|||
Melt Temperature | 215 - 250 °C | 419 - 482 °F | |
ExxonMobil Santoprene® 8291-65TB Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic elastomer which bonds to adhesive/epoxy spin-finished polyester or standard nylon fibers for closed-braid hose and woven-substrate products. With bonds strong.. |
|||
Melt Temperature | 215 - 225 °C | 419 - 437 °F | |
NOVA Chemicals Sclair® 10B Octene VLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent sealability, excellent dart impact, excellent clarity.Applications: Co-extrusion.Data provided by the manufacturer. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 100TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100TL NC010 is a high viscosity acetal homopolymer with 1.5% Teflon® PTFE Micropowder.Information provided by DuPont Performance Polymers |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability, low die deposit, and enhanced crystallization for low porosity.Information pr.. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 311DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 311DP BK402 is a medium high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding(reduced warpage, less shrinkage, fewer voids).Informatio.. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 511DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided.. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 911DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by.. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® FG500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500AL is a medium viscosity acetal homopolymer, lubricated for low wear and /or coefficient of friction. It has been developed for consideration into applications such as parts for the fo.. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500TL medium viscosity acetal homopolymer resin containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.In.. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG511DP is a medium viscosity acetal homopolymer, with improved thermal stability and modifications for more precise molding. It has been developed for consideration into applications such .. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov.. |
|||
Melt Temperature | 215 - 240 °C | 419 - 464 °F | |
Ineos ABS Lustran® 256 Extrusion, Blending
(discontinued **) A natural, medium-flow, medium-impact extrusion grade of ABS. It is used for blending with other Lustran ABS virgin and regrind materials to optimize cost and performance.Properties tested in trans.. |
|||
Melt Temperature | 215 - 240 °C | 419 - 464 °F | |
Ineos ABS Lustran® 356 Extrusion, Low-Gloss
(discontinued **) Properties tested in transverse direction (worst case) on 125-mil (3.2 mm) extruded sheets specimens with |
|||
Melt Temperature | 215 - 240 °C | 419 - 464 °F | Injection Molding |
LG Chemical KEYFLEX BT 1068D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 215 - 245 °C | 419 - 473 °F | Injection Molding |
LG Chemical KEYFLEX BT 3047D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 215 - 245 °C | 419 - 473 °F | Extrusion Molding |
LG Chemical KEYFLEX BT 3047D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melt Temperature | 215 - 250 °C | 419 - 482 °F | Injection Molding |
LG Chemical LUMID GP1300AP PA6, Plasticized Feature: Injection Molding, PA6, PlasticizedApplication: Automotive PartsInformation provided by LG Chemical |
|||
Melt Temperature | 215 - 249 °C | 419 - 480 °F | Extrusion |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
Melt Temperature | 215 °C | 419 °F | Recommended Injection Molding |
MBA Polymers ABS 4124 Recycled acrylonitrile-butadiene-styrene copolymer Available in standard black.Information provided by MBA Polymers. |
|||
Melt Temperature | >= 215 °C | >= 419 °F | |
Voloknohim Nylon 6 Chips A Grade Packing: Nylon 6 is packed in 650 kg big-bags on palletsInformation provided by Voloknokhim |
|||
Melt Temperature | 215 °C | 419 °F | Injection |
Lubrizol ESTANE® 58132 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUses: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
Melt Temperature | >= 215 °C | >= 419 °F | |
Voloknohim PA 6-210/310 Nylon 6 For production of plastics and industrial goods used in machine building and motor industry. Nylon 6 bright, not dyed and (or) heat stabilizedInformation provided by Voloknokhim |
|||
Melt Temperature | 215 - 235 °C | 419 - 455 °F | |
Covestro Desmopan® DP 3660DU Polyurethane Extrusion- and injection molding gradetransparent up to 6 mm wall thicknesshydrolysis-stabilisedwith special UV stabilizerswith release agentgood wear resistanceApplicationSports shoe solesHosesnon-.. |
|||
Melt Temperature | 215 °C | 419 °F | 90 RPM |
Equate EMDA-6200 HDPE Blow Molding Resin EMDA-6200 grade is a high-density polyethylene copolymer resin designed for blow molding small to medium size bottles. It can be used on intermittent as well as continuous blow molding machines for .. |
|||
Melt Temperature | 215 - 225 °C | 419 - 437 °F | |
E-Polymers SEPAZ® LH40 PP Homopolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Melt Temperature | 215 - 225 °C | 419 - 437 °F | |
E-Polymers SEPAZ® LC40 PP Copolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® FG100TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100TL is a high viscosity acetal homopolymer, containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.Inform.. |
|||
Melt Temperature | 215 °C | 419 °F | Optimum; Injection Molding |
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by.. |