Extrusion- and injection molding gradevery good hydrolysis and microbial resistancegood low-temperature flexibilitycomplies with VDE 0282-10ApplicationCable sheathingsHosesnon-reinforcedPreprocessingMax. Water content
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
Melt
1.11 g/cc
0.0401 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
3s; ISO 868
Hardness, Shore D 31
31
15s; ISO 868
Abrasion 20
20
mm³; ISO 4649
Compression Set 25 %

@Temperature 23.0 °C
25 %

@Temperature 73.4 °F
ISO 815
42 %

@Temperature 70.0 °C
42 %

@Temperature 158 °F
ISO 815
Thermal Properties Metric English Comments
Specific Heat Capacity 1.70 J/g-°C
0.406 BTU/lb-°F
Melt
Thermal Conductivity 0.129 W/m-K
0.895 BTU-in/hr-ft²-°F
Melt
Processing Properties Metric English Comments
Melt Temperature 205 - 225 °C
401 - 437 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Ejection Temperature 50.0 °C
122 °F
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
India
Near East/Africa
South and Central America
Eff. thermal diffusivity (m²/s) 8E-08