E-Polymers SEPAZ® LH40 PP Homopolymer LFT Resin

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer E-Polymers Co. Ltd.
Trade Name SEPAZ®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers SEPAZ® LH40 PP Homopolymer LFT Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and delivers optimal reinforcement to the plastic matrix in contrast to conventional short glass fiber-reinforced thermoplastics. Molded parts made of SEPAZ LFT are used in virtually every sector of consumer and industrial manufacturing, including automotive, recreation & sports, marine, food & beverage.Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Water Absorption 0.020 %

@Time 86400 sec
0.020 %

@Time 24.0 hour
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength 117.72 MPa
17074 psi
ASTM D638
Elongation at Break 2.5 %
2.5 %
ASTM D638
Flexural Strength 181.49 MPa
26323 psi
ASTM D790
Flexural Modulus 8.3385 GPa
1209.4 ksi
ASTM D790
Izod Impact, Notched 2.94 J/cm

@Temperature 23.0 °C
5.51 ft-lb/in

@Temperature 73.4 °F
ASTM D256
2.94 J/cm

@Temperature -30.0 °C
5.51 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
Flammability, UL94 HB
HB
Processing Properties Metric English Comments
Melt Temperature 215 - 225 °C
419 - 437 °F
Mold Temperature 40.0 - 70.0 °C
104 - 158 °F