Polymer Property : Nozzle Temperature = 290 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Nozzle Temperature 245 - 290 °C
473 - 554 °F
Nilit Nilamid B3 H G7 35% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G7 is a general purpose, 35% glass fiber reinforced NYLON 6. It has high mechanical performance, and also excellent moldability. Its impact performance is outstanding, so i..
Nozzle Temperature 245 - 290 °C
473 - 554 °F
Nilit Nilamid B3 H G8 40% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G8 is a product that combines outstanding strength and stiffness with good moldability and good impact strength. It is widely used for structural applications.Key character..
Nozzle Temperature 275 - 290 °C
527 - 554 °F
Nilit Nilamid A3 H ZE High Impact PA66
Description: Nilamid A3 H ZE was developed for applications which are subjected to very high shock loads, also at minus temperatures. It has good impact performance, whilst maintaining good strength..
Nozzle Temperature 245 - 290 °C
473 - 554 °F
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha..
Nozzle Temperature 270 - 290 °C
518 - 554 °F
Injection Molding
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant
Feature: Injection Molding, PA66+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
Nozzle Temperature 260 - 290 °C
500 - 554 °F
Injection Molding
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose
Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Nozzle Temperature 260 - 290 °C
500 - 554 °F
Injection Molding
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose
Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Nozzle Temperature 260 - 290 °C
500 - 554 °F
Injection Molding
LG Chemical LUMID GP2330A(W) PA6+GF33%, General Purpose
Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Cooling Fan), E&E (Bobbin)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
Nozzle Temperature 280 - 290 °C
536 - 554 °F
Injection Molding
LG Chemical LUMID SG4389B PA66+GF/MF38%
Feature: Injection Molding, PA66+GF/MF38%Application: Automotive (Fan & Shroud)CAS No. 32131-17-2, 25038-54-4, 65997-17-3 and 14807-96-6Information provided by LG Chemical
Nozzle Temperature 250 - 290 °C
482 - 554 °F
LG Chemical LUPOY GP-5200 General Purpose PC/ABS Alloy, 10% Polymer Alloy, High Strength
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Nozzle Temperature 250 - 290 °C
482 - 554 °F
LG Chemical LUPOY GP-5300 General Purpose PC/ABS Alloy, 30% Polymer Alloy, High Strength, Dimensional Stability
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Nozzle Temperature 250 - 290 °C
482 - 554 °F
LG Chemical LUPOY GP-5306F General Purpose PC/ABS Alloy, 30% Polymer Alloy, Weather Resistant, Flame Retardant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Nozzle Temperature 270 - 290 °C
518 - 554 °F
LG Chemical LUPOY HI-1002 High Impact Modified PC, Unreinforced
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..
Nozzle Temperature 280 - 290 °C
536 - 554 °F
Solvay Technyl® A218 Heat Stabilized Nylon 66
Information provided by Rhodia; Rhodia has been acquired by Solvay.
Nozzle Temperature 260 - 290 °C
500 - 554 °F
Solvay Specialty Polymers Ixef® 1032 Polyarylamide (PARA), 60% Glass Fiber (Conditioned)
Ixef® 1032 is a 60% glass-fiber reinforced, general purpose polyarylamide compound which exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Featur..
Nozzle Temperature 260 - 290 °C
500 - 554 °F
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without s..
Nozzle Temperature 280 - 290 °C
536 - 554 °F
Tisan TISARBON® Flame Retardant (V0) Polycarbonate
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind..
Nozzle Temperature 280 - 290 °C
536 - 554 °F
Tisan TISARBON® UNR Polycarbonate
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind..
Nozzle Temperature 230 - 290 °C
446 - 554 °F
Arkema Group Pebax® 6333 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
Nozzle Temperature 230 - 290 °C
446 - 554 °F
Arkema Group Pebax® 6333 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
Nozzle Temperature 230 - 290 °C
446 - 554 °F
Arkema Group Pebax® 7033 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 7033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
Nozzle Temperature 230 - 290 °C
446 - 554 °F
Arkema Group Pebax® Rnew 63R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 63R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
Nozzle Temperature 230 - 290 °C
446 - 554 °F
Arkema Group Pebax® Rnew 72R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 72R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
Nozzle Temperature 240 - 290 °C
464 - 554 °F
Arkema Group Rilsan® PA 11 G BMNO MED Nylon 11
Rilsan® PA 11 G BMNO MED is a polyamide produced from a renewable source. This grade offers the highest quality and it is specially designed to meet the stringent requirements of the medical applic..
Nozzle Temperature 260 - 290 °C
500 - 554 °F
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM
Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m..
Nozzle Temperature 270 - 290 °C
518 - 554 °F
Celanese Impet® Hi430 15% Glass Filled, Impact Modified PET
Description: Impet Hi 430 is a 15% glass filled and impact modified PET which has an excellent balance of mechanical properties as well as excellent processability and surface appearance.Information..
Nozzle Temperature 260 - 290 °C
500 - 554 °F
Ascend Performance Materials Vydyne® ECO366 Nylon 66, Flame-retardant, DAM
Vydyne® ECO366 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for machin..
Nozzle Temperature 180 - 290 °C
356 - 554 °F
Average value: 238 °C Grade Count:34
Overview of materials for Polyether Block Amide (PEBA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Block Amide (PEBA)". Each property range of values reported is minimum and maximum values of a..
Nozzle Temperature 275 - 290 °C
527 - 554 °F
Celanese Impet® 830R PET, 35% Mineral / Glass Reinforced  (Unverified Data**)
Impet 830R is a 35% glass/mineral reinforced injection moldable polyester made with recycled PET. It provides an excellent combination of strength, stiffness, warp resistance, and high temperature c..
Nozzle Temperature 270 - 290 °C
518 - 554 °F
LG Chemical LUPOY SR-3108F High Flow Modified PC, 10% Mineral Fillers, High Reflectivity, Flame Retardant
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive..