Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 1-1120 Polyamide 66, with PTFE, lubricant modified, high viscosity Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 1-7139 Polyamide 66, with aramid reinforcement and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Emergency running property.Improved heat resistance.Control disks, cams, sliding elements and o.. |
|||
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 1-8521 Polyamide 66, with carbon fiber and glass fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Nozzle Temperature | 280 - 330 °C | 536 - 626 °F | |
Lehmann & Voss LUVOCOM® 19-7660 Polyamide 46, with glass fiber, PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Highly dimensionally stable at elevated temperatures.Gear parts for automot.. |
|||
Nozzle Temperature | 280 - 330 °C | 536 - 626 °F | |
Lehmann & Voss LUVOCOM® 19-8074 Polyamide 46, with aramid reinforcement and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Good friction and wear behaviour especially at increased temperatures.Emergency running propert.. |
|||
Nozzle Temperature | 280 - 330 °C | 536 - 626 °F | |
Lehmann & Voss LUVOCOM® 19-8263 Polyamide 46, with carbon fiber and glass fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Electrically conductive, suitable for continuous discharging of statically generated electricit.. |
|||
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F | Injection Molding |
LG Chemical LUCON PO6062 mPPO+CNT+CF+GF Description: Injection Molding, mPPO+CNT+CF+GF, High Strength, Heat StabilityApplication: ATM parts, LCD Cell TrayCAS No. 35134-01-4, 25038-54-4, 65997-17-3, 7440-44-0 and 7782-42-5Information provi.. |
|||
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 1/CF/10/GF/20/BK Polyamide 66, with carbon fiber and glass fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/HS/BK Polyamide 66, with glass fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low warpage.Improved friction and wear behaviour. Emergency running propert.. |
|||
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/HS-B Polyamide 66, with glass fiber and PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Heat stabilised.High dimension.. |
|||
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 1/GF/30/TF/15/SI/2-2 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 1-1108 Polyamide 66, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 1-1129 Polyamide 66, with glass fiber, PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Strong, stiff parts.Bearings, .. |
|||
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 1-3260/schwarz Polyamide 66, with PTFE, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 1-7180/EG Polyamide 66, with carbon fiber, PTFE, lubricant modified, high viscosity, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Nozzle Temperature | 280 - 330 °C | 536 - 626 °F | |
Lehmann & Voss LUVOCOM® 19-7745 Polyamide 46, with PTFE, improved wear resistance Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Good friction and wear behaviour especially at increased te.. |
|||
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOTECH® GS 58 Polyamide 66, with glass fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec.. |
|||
Nozzle Temperature | 280 - 310 °C | 536 - 590 °F | Injection Molding |
LG Chemical LUSEP SP2300 SPS+GF30%, General Purpose Feature: Injection Molding, sPS+GF30%, General PurposeApplication: Pump Units, Pick-up Lends Holder, etc.CAS No. 9003-53-6 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 280 - 295 °C | 536 - 563 °F | |
Akro-Plastic Akromid® A3 GF 60 (2424) PA 6.6 Dry, 60% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F | |
Ascend Performance Materials Vydyne® 21SPC Nylon 66, DAM Vydyne® 21SPC is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding fabrication. This resin offers a well balanced combination of engineering .. |
|||
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F | |
Ascend Performance Materials Vydyne® 21SPF Nylon 66, General Purpose, High Productivity, DAM Vydyne® 21SPF is general-purpose PA66 resin. Available in natural, it is designed principally for injection-molding fabrication. This grade offers a well-balanced combination of engineering propert.. |
|||
Nozzle Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R220 Nylon 66, 40% mineral reinforced, DAM Vydyne® R220 is a 40% mineral-reinforced PA66 resin formulated for improved impact strength. Available in natural, it is an injection-molding grade formulated to retain the inherent processing adva.. |
|||
Nozzle Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R543H Natural Nylon 66, 43% Glass Reinforced, DAM Vydyne® R543H Natural is general-purpose, hydrolysis-resistant, 43% glass-fiber reinforced PA66 resin. Available in natural, it is an injection-molding grade resin that is lubricated for machine fe.. |
|||
Nozzle Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R550 Nylon 66, 50% Glass Reinforced, DAM Vydyne® R550 is general-purpose, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is also lubricated for improved flow and offers superior surface appearance. G.. |
|||
Nozzle Temperature | 280 - 295 °C | 536 - 563 °F | |
Akro-Plastic Akromid® A3 GF 20 (2419) PA 6.6 Dry, 20% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Nozzle Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 41H NT Nylon 66, Impact Modified, DAM Vydyne® 41H NT is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyn.. |
|||
Nozzle Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® 41 NT Nylon 66, Impact Modified, DAM Vydyne® 41 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Nozzle Temperature | 280 - 310 °C | 536 - 590 °F | |
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Nozzle Temperature | 280 - 300 °C | 536 - 572 °F | |
Lehmann & Voss LUVOCOM® 1-0865 Polyamide 66, with aramid reinforcement, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Improved heat resistance.Control disks, cams, sliding elements and other duty parts.. |
|||
Nozzle Temperature | 280 - 320 °C | 536 - 608 °F | Injection Molding |
LG Chemical LUXY KS G55 Amorphous PA6 Description: Injection Molding, Amorphous PA6, High Modulus, High Impact, Low WarpageApplication: Electric/Electronic Components (LCD Bracket)Information provided by LG Chemical |