NHEP Spectron™ E6126 Nylon 66, 20% Glass Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 20% Glass Fiber Filled
Manufacturer Ngai Hing Hong Engineering Plastic (Hong Kong) Ltd .
Trade Name Spectron™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NHEP Spectron™ E6126 Nylon 66, 20% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Natural color. E6126 exhibits high rigidity, mechanical strength, and excellent appearance. It is suitable for wide range of applications.Property data measured at room temperature, 50% RH.Information provided by Bieglo Gmbh for Ngai Hing Engineering Plastic (Hong Kong) Ltd.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 110 MPa
16000 psi
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Flexural Strength 160 MPa
23200 psi
ASTM D790
Flexural Modulus 5.00 GPa
725 ksi
ASTM D790
Izod Impact, Notched 0.400 J/cm
0.749 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 225 °C
437 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 250 - 260 °C
482 - 500 °F
Middle Barrel Temperature 260 - 270 °C
500 - 518 °F
Front Barrel Temperature 270 - 280 °C
518 - 536 °F
Nozzle Temperature 280 - 290 °C
536 - 554 °F
Mold Temperature 100 - 120 °C
212 - 248 °F
Drying Temperature 100 - 120 °C

@Time 7200 - 14400 sec
212 - 248 °F

@Time 2.00 - 4.00 hour
Descriptive Properties Value Comments
Processing Injection Pressure Medium-High
Processing Injection Speed Medium-High