Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LG Chemical LUPOY GP-5200 General Purpose PC/ABS Alloy, 10% Polymer Alloy, High Strength

Category Polymer , Thermoplastic , ABS Polymer , Polycarbonate (PC)
Manufacturer LG Chemical
Trade Name LUPOY
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical LUPOY GP-5200 General Purpose PC/ABS Alloy, 10% Polymer Alloy, High Strength.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Among the characteristics of LUPOY polycarbonate resins are excellent mechanical properties, high heat resistance, high impact strength, and dimensional stability.Applications:Automotive: Automotive front ends, cluster pad main panel (instrument panel), lower cluster pad main, console box, glove box cover, door, wheel cover and cap, defroster grill, back mirror housingElectrical and Electronic: Monitor housing, fax housing, notebook PC housing, cellular phone case, fax and copy machine frame, CD ROM drive tray and main frame, relay case, connector, switchIndustrial Parts and Household Appliance: Helmet, terminal box, electrical tool housing, industrial bobbin, distributing board box, power tool component, gears and cams, water meter housingInformation Provided by LG Chem
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 116
116
ASTM D785
Tensile Strength, Yield 98.0 MPa
14200 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 137 MPa
19900 psi
ASTM D790
Flexural Modulus 5.29 GPa
767 ksi
ASTM D790
Izod Impact, Notched 0.980 J/cm

@Temperature 23.0 °C
1.84 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 120 °C
248 °F
ASTM D648
Processing Properties Metric English Comments
Rear Barrel Temperature 230 - 270 °C
446 - 518 °F
Middle Barrel Temperature 240 - 280 °C
464 - 536 °F
Front Barrel Temperature 250 - 290 °C
482 - 554 °F
Nozzle Temperature 250 - 290 °C
482 - 554 °F
Melt Temperature 260 - 300 °C
500 - 572 °F
Mold Temperature 70.0 - 110 °C
158 - 230 °F
Drying Temperature 70.0 - 100 °C
158 - 212 °F
Dry Time 3 - 5 hour
3 - 5 hour
Screw Speed 40 - 70 rpm
40 - 70 rpm