Tisan TISARBON® UNR Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Tisan Engineering Plastics
Trade Name TISARBON®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tisan TISARBON® UNR Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products industries. General Specifications include: High temperature resistanceDimensional stabilityImpact resistanceExcellent surface qualityHigh light transparenceFlame resistanceLow moisture ratioToughness TISARBON has good chemical resistance against weak acids. It has medium resistance against alcohols, hydrocarbons, and engine fuels, and weak resistance against acids, alkalis, and organic solvents.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Linear Mold Shrinkage 0.0070 cm/cm
0.0070 in/in
Melt Flow 22 g/10 min
22 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 91
91
ISO 868
Tensile Strength at Break 65.0 MPa
9430 psi
ISO 527-2
Tensile Strength, Yield 65.0 MPa
9430 psi
ISO 527-2
Elongation at Break 12 %
12 %
ISO 527-2
Elongation at Yield 9.0 %
9.0 %
ISO 527-2
Modulus of Elasticity 2.00 GPa
290 ksi
ISO 527-2
Izod Impact, Notched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 230 °C
446 °F
Vicat Softening Point 150 °C
302 °F
ISO 306
Heat Distortion Temperature 145 °C
293 °F
ISO 75-2
Flammability, UL94 V-2
V-2
Glow Wire Test 750 °C
1380 °F
60695-2-10
Electrical Properties Metric English Comments
Comparative Tracking Index 400 V
400 V
TS EN 60112
Processing Properties Metric English Comments
Feed Temperature 70.0 °C
158 °F
Rear Barrel Temperature 280 - 290 °C
536 - 554 °F
Aft-1. Region Temperature
Middle Barrel Temperature 270 - 280 °C
518 - 536 °F
Mid-2. Region Temperature
Front Barrel Temperature 260 - 270 °C
500 - 518 °F
Pre-3. Region Temperature
Nozzle Temperature 280 - 290 °C
536 - 554 °F
Melt Temperature 270 - 290 °C
518 - 554 °F
Drying Temperature 90.0 - 120 °C
194 - 248 °F
Predrying Temperature
Dry Time 3 - 5 hour
3 - 5 hour
Predrying Time
Moisture Content 0.20 %
0.20 %
ISO 62
Descriptive Properties Value Comments
Block Temperature 80°C