Processing Properties | Metric | English | Comments |
---|---|---|---|
Nozzle Temperature | 260 - 275 °C | 500 - 527 °F | |
Parker Chomerics PREMIER™ A230-ST EMI Shielding Plastic Description: PREMIER™ is the world’s first and most versatile commercially available conductive thermoplastic for real world EMI shielding solutions. It is a blend of PC/ABS thermoplastic polymer .. |
|||
Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
LG Chemical LUMID GP2300A(W) PA6+GF30%, General Purpose Feature: Injection Molding, PA6+GF30%, General PurposeApplication: Automotive (Side Mirror Base Plate)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | Injection Molding |
LG Chemical LUMID GP2330A(W) PA6+GF33%, General Purpose Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Cooling Fan), E&E (Bobbin)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical |
|||
Nozzle Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
LG Chemical LUMID GP3400A(W) PA6+MF40%, General Purpose Feature: Injection Molding, PA6+MF40%, General PurposeApplication: E&E (Rice Cooker Housing)CAS No. 25038-54-4 and 14807-96-6Information provided by LG Chemical |
|||
Nozzle Temperature | 260 - 275 °C | 500 - 527 °F | Injection Molding |
LG Chemical LUMID HI5083A(W) PA6/ABS+MF8%, High Impact Feature: Injection Molding, PA6/ABS+MF8%, High ImpactApplication: Electric/Electronic Components (Shaver Die)CAS No. 25038-54-4, 9003-56-9, 9003-54-7 and 14807-96-6Information provided by LG Chemica.. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | Injection Molding |
LG Chemical Lupox® TE5000SZ PBT+PC Description: Injection Molding, PBT+PC, High Impact, Dimensional StabilityApplication: Automotive ItemCAS No. 137050-02-03, 26062-94-2 and 103598-77-2Information provided by LG Chemical |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | |
Gromax PBT 3030-201 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | |
Gromax PBT 5130-104 30% Glass Fiber Filled CCP Halogen-free PBT, Black. PBT flame-retarded glass fiber 30% reinforced injection molding gradeCharacteristics:Excellent electrical property Excellent temperature resistance, high heat distortion.. |
|||
Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
LTL Color Compounds ColorFast® NY2GF330 Nylon 66, 33% Glass-Filled 33% glass-filled nylon 6,6All information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 260 - 275 °C | 500 - 527 °F | Injection Molding |
LG Chemical LUPOY GN5151RF PC/ABS Mineral Filler Description: Injection Molding, PC/ABS Mineral Filler, General Purpose, High Stiffness, Halogen Free Flame RetardantApplication: E&E (Housing), IT/OA (Notebook PC Housing)CAS: 103598-77-2, 9003-56-9.. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | |
Gromax PBT 3015-201 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | |
Gromax PBT 3030-104 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® DW-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® DW-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® FC-1022 Polyarylamide (PARA), 50% Glass Fiber (Conditioned) Ixef® FC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® FC-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® FC-1022 is a 50% glass-fiber reinforced, general purpose polyarylamide compound that exhibits very high strength and rigidity, outstanding surface gloss, and excellent creep resistance.Feat.. |
|||
Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | |
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry) Ixef® GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without s.. |
|||
Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
Wellman Wellamid® GS25-66 22LH-N 25% Glass Sphere Filled Nylon 66, Lubricated & Heat Stabilized Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
Wellman Wellamid® GS25-66 22L-N, 25% Glass Sphere Filled Nylon 66, Lubricated Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided.. |
|||
Nozzle Temperature | 260 °C | 500 °F | Recommended |
Arkema Group Pebax® 7033 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® 7033 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t.. |
|||
Nozzle Temperature | 260 °C | 500 °F | Recommended |
Arkema Group Pebax® Rnew 72R53 SP 01 Polyether Block Amide (PEBA) Polyether block amide Pebax® 72R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV.. |
|||
Nozzle Temperature | 260 - 290 °C | 500 - 554 °F | |
Ascend Performance Materials Vydyne® ECO315 BK13 Nylon 66, Flame Retardant, DAM Vydyne® ECO366 BK13 is a non-halogenated, unfilled, flame-retardant PA66 homopolymer designed with superior flow properties to assist in filling thin-walled, intricate parts. It is lubricated for m.. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | |
Gromax CCP PBT 4815-NCB 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Nozzle Temperature | 260 - 265 °C | 500 - 509 °F | |
Beijing Chemical Industry KAIFA® MN101 Nylon 66 Resin Good flow, High impactInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Nozzle Temperature | 260 - 288 °C | 500 - 550 °F | |
LTL Color Compounds ColorFast® NY1GF330 Nylon 6, 33% Glass-Filled 33% glass-filled nylon 6All information provided by LTL Color Compounders, Inc. |
|||
Nozzle Temperature | 260 °C | 500 °F | |
Tipco Tipcofil® AGM 802 - 25% Mineral & 15% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 25% Mineral + 15% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | |
Gromax CCP PBT 5615-104C 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Nozzle Temperature | 260 - 270 °C | 500 - 518 °F | |
Gromax CCP PBT 5630-104C 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Nozzle Temperature | 260 - 280 °C | 500 - 536 °F | |
Gromax CCP PET 9130-200 30% Glass Filled Product Description: PET glass/mineral 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excell.. |
|||
Nozzle Temperature | 260 - 280 °C | 500 - 536 °F | Injection Molding |
LG Chemical LUMID GP3300A(W) PA6+MF30%, General Purpose Feature: Injection Molding, PA6+MF30%, General PurposeApplication: Automotive (Battery Pack Housing)Information provided by LG Chemical |