Processing Properties Metric English Comments
Processing Temperature 163 °C
325 °F
Ejection temperature; Internal
C 52021 POM  (Unverified Data**)
Chemical abbreviation according to ISO 1043-1: POMInjection molding grade with extremely high flowInformation provided by Celanese
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming Temperature
Kleerdex Kydex® 130 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Decorative thermoplastic sheetApplications: Appliances, laminations, electronics, in-store displays, medical devices, equipment housings, dental equipmentFeatures: For deep to hard to form parts or ..
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming Temperature
Kleerdex Kydex® L Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Laminating grade fire rated sheetApplications: Store fixtures and displays, exhibits, service counters, doors, partitionsFeatures: Toughness and durability, solid, integral color, chemical resistanc..
Processing Temperature 163 °C
325 °F
Cure Schedule: 20 min @ 163°C
Huntsman HT 9690 Special Hardener
Mix Ratio with ECN 1299 is 50.Comments/Applications: 0-cresol novolac hardener. *Mix ratio with ECN 1299. Latent with ECN resins. High temperature resistant. Molding compound and powder coatin..
Processing Temperature 163 - 204 °C
325 - 399 °F
Thermoforming
KYDEX® 430 ABS/PVC Blend for Medical Device Housings
KYDEX® 430 is an ABS/PVC thermoplastic sheet that offers superior thermoformability, rigidity, breakage resistance, chemical resistance and fire retardancy.Features:Good for deep or hard to form ..
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming
KYDEX® 6503 Integral Pearlescent Low Heat Release Aviation Thermoforming Sheet
Features:Thicknesses from 0.71 mm to 3.18 mmChemical resistant - easy to clean with aggressive cleanersForms deep draws with low forces when heated to the upper end of forming temperature rangeCrisp..
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming Temperature
KYDEX® 6185 Thermoplastic Sheet
High temperature aircraft gradeApplications: Aircraft interior components examples include: air ducts, window reveals, instrument panels, toilet shrouds, armrestsFeatures: Kydex 6185 is a proprietar..
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming Temperature
KYDEX® 6565 Acrylic/PVC Thermoplastic Sheet
Low heat release aviation gradeApplications: Airducts, seat parts, bulkhead laminates, escape slide packboards, gallery parts, instrument panels, laboratory floorplans, sidewall panels, life vest sh..
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming
KYDEX® 6565(d) Decorative Low Heat Release Thermoplastic Sheet, Aviation
Features:Wide range of thicknesses availableVery resistance to a wide range of concentrate chemicals, easy to cleanForms to deep draws with low forces when heated to the upper end of the proper form..
Processing Temperature 163 - 174 °C
325 - 345 °F
Recommended Stock Temperature
Sylvin Technologies 5132-75 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-001 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-003 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-005 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-026 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-028 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-046 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-050 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-051 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-082 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-085 Clear Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-091 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-116 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 168 °C
325 - 335 °F
Axiall 3020 Rigid PVC, Extrusion
Georgia Gulf 3020 is a base for use of wood flour up to 40 percent. Impact strength and toughnessFlame retardantChemical resistanceDimensional stabilityInformation provided by Georgia GulfGeorgia G..
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
CPT C-Flex® R70-190 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Processing Temperature 163 - 199 °C
325 - 390 °F
RTP Company PermaStat® 1200-70A  Polyurethane Thermoplastic Elastomer (TPU) Anti-Static - 70 Shore A
Anti-Static - 70 Shore AComments:Permanently Anti-StaticESD Protection70-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect propert..
Processing Temperature 163 - 199 °C
325 - 390 °F
RTP Company PermaStat® 1200-75A  Polyurethane Thermoplastic Elastomer (TPU) Anti-Static - 75 Shore A
Anti-Static - 75 Shore AComments:Permanently Anti-StaticESD Protection75-A DurometerUnless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect propert..
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming Temperature
Kleerdex Kydex® 100 AS Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Anti-static sheetApplications: Housings for equipment such as photocopy machines, instrument panels, computers, keyboards, telephones, internal parts for electrical and electronic equipment, medical..
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming Temperature
Kleerdex Kydex® 200 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
General purpose gradeApplications: Can be used to substitute effectively for both general purpose ABS and acrylic/PVC thermoplastics. Examples include data processing equipment housings, photocopy ..
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming Temperature
Kleerdex Kydex® 510 Acrylic/PVC Thermoplastic Sheet  (discontinued **)
Weatherable and decorative sheetApplications: Housings for equipment, recreation vehicles and truck parts, safety equipment, building products, signage, wall panels, facia, doors, service counters, ..
Processing Temperature 163 - 174 °C
325 - 345 °F
Recommended Stock Temperature
Sylvin Technologies 5123 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.