Huntsman HT 9690 Special Hardener

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman HT 9690 Special Hardener.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Mix Ratio with ECN 1299 is 50.Comments/Applications: 0-cresol novolac hardener. *Mix ratio with ECN 1299. Latent with ECN resins. High temperature resistant. Molding compound and powder coatings.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 - 110 °C
212 - 230 °F
Softening Range
Processing Properties Metric English Comments
Processing Temperature 163 °C
325 °F
Cure Schedule: 20 min @ 163°C