Polymer Property : Processing Temperature = 168 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 157 - 168 °C
315 - 335 °F
Recommended Stock Temperature
Sylvin Technologies 5100 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Processing Temperature 163 - 168 °C
325 - 335 °F
Axiall 3014 Rigid PVC, Extrusion
Georgia Gulf 3014 is a base for use of wood flour up to 40 percent. Impact Strength & ToughnessFlame RetardantChemical ResistanceDimensional StabilityInformation provided by Georgia GulfGeorgia Gul..
Processing Temperature 163 - 168 °C
325 - 335 °F
Axiall 3020 Rigid PVC, Extrusion
Georgia Gulf 3020 is a base for use of wood flour up to 40 percent. Impact strength and toughnessFlame retardantChemical resistanceDimensional stabilityInformation provided by Georgia GulfGeorgia G..