Category Polymer , Thermoplastic
Manufacturer KYDEX LLC
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KYDEX® 6565(d) Decorative Low Heat Release Thermoplastic Sheet, Aviation.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Wide range of thicknesses availableVery resistance to a wide range of concentrate chemicals, easy to cleanForms to deep draws with low forces when heated to the upper end of the proper forming temperature rangeCrisp detail, minimal rejectsCan be formed on all standard presses and cut on all standard die-cutting machinesSecondary operations include: machining, sawing, blanking, punchingSuggested Applications:Seat partsBulkhead laminatesLife vest shroudsPassenger service unitsMonitor shroudsArmrestsWindow shadesMolding stripsTray tablesKick panelsInformation provided by Kydex, LLC.
Physical Properties Metric English Comments
Specific Gravity 1.52 g/cc
1.52 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 111
111
ASTM D785
Tensile Strength 43.0 MPa
6240 psi
ASTM D638
Flexural Strength 81.2 MPa
11800 psi
ASTM D790
Flexural Modulus 3.833 GPa
555.9 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 75.9 °C
169 °F
annealed; ASTM D648
Processing Properties Metric English Comments
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming
Descriptive Properties Value Comments
Federal Aviation Administration < 65/65
FAR 25.853 (d); Rate of Heat Release
Pass
FAR 25.853 (a)
Pass
FAR 25.853 (d); Smoke Generation
Users viewing this material also viewed the following: