Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CPT C-Flex® R70-091 Opaque Biocompatible TPE

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Consolidated Polymer Technologies
Trade Name C-Flex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CPT C-Flex® R70-091 Opaque Biocompatible TPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current United States Pharmacopoeia Class VI test requirements. C-Flex® does not contain latex rubber, polyvinyl chloride, silicone rubber, or polyurethane.Information provided by Consolidated Polymer Technologies.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D 792
Linear Mold Shrinkage 0.018 - 0.020 cm/cm
0.018 - 0.020 in/in
Melt Flow 8.7 g/10 min
8.7 g/10 min
Condition S; ASTM D 1238
Mechanical Properties Metric English Comments
Hardness, Shore A 51
51
1 sec.; ASTM D 2240
Tensile Strength at Break 9.935 MPa
1441 psi
ASTM D 412
Elongation at Break 756 %
756 %
ASTM D 412
100% Modulus 0.000896 GPa
0.130 ksi
ASTM D 412
300% Modulus 0.00172 GPa
0.250 ksi
ASTM D 412
Tear Strength 42.4 kN/m
242 pli
Die C; ASTM D 624
52.9 kN/m
302 pli
Notched, Die B; ASTM D 624
Taber Abrasion, mg/1000 Cycles 159.3
159.3
Federal Test Method Standard, 405
Compression Set 38 %
38 %
23°C; ASTM D 412
85 %

@Temperature 70.0 °C
85 %

@Temperature 158 °F
ASTM D 412
Tensile Set 11 %
11 %
at 300% elongation; ASTM D 412
46 %
46 %
at break; ASTM D 412
Processing Properties Metric English Comments
Processing Temperature 163 - 204 °C
325 - 400 °F
Extrusion Temperature
Middle Barrel Temperature 149 - 218 °C
300 - 425 °F
Injection molding cylinder temperature
Drying Temperature 65.6 - 93.3 °C
150 - 200 °F
Desiccant type
Injection Pressure 2.07 - 6.89 MPa
300 - 1000 psi
Descriptive Properties Value Comments
Sterilization methods: Cobalt 60, Ethylene Oxide
Steam/Autoclave not recommended
Copyright © lookpolymers.com All Rights Reserved