Material Notes:
General purpose gradeApplications: Can be used to substitute effectively for both general purpose ABS and acrylic/PVC thermoplastics. Examples include data processing equipment housings, photocopy machines, vending machine chutes, and consumer products.Features: It is among the most rigid of thermoforming materials as demonstrated by its high modulus of elasticity. Particularly effective fro pressure forming and/or where the part is going to be painted. Meet the requirement so f94 V-0 in all gauges as tested by an independent lab. Provides excellent extensibility, good impact resistance, and excellent solvent resistance. Radiant Panel: 35 as per ASTM E162Fabrication: Excellent forming properties result in uniform wall thicknesses and crisp detail, plus easy machining and fabricating using conventional methods, further expanding finished part possibilities.Data provided by the Kleerdex Company.Kleerdex Company became KYDEX, LLC in 2009.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
0.0040 - 0.0060 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell R 94
94
ASTM D785
Tensile Strength, Ultimate 42.0 MPa
6090 psi
ASTM D638
Elongation at Break 80 %
80 %
Modulus of Elasticity 2.206 GPa
320.0 ksi
Flexural Yield Strength 63.0 MPa
9140 psi
ASTM D790
Izod Impact, Notched 5.34 J/cm

@Temperature 23.0 °C
10.0 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
annealed; ASTM D648
Flammability, UL94 V-0
V-0
Independent Test Lab
Processing Properties Metric English Comments
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming Temperature