Material Notes:
KYDEX® 430 is an ABS/PVC thermoplastic sheet that offers superior thermoformability, rigidity, breakage resistance, chemical resistance and fire retardancy.Features:Good for deep or hard to form partsMore rigid, parts will deform less when loaded, can be down -gauged for weight savingsUniform wall thickness and crisp detailLow moisture absorption - no drying needed prior to thermoformingEasy machining and fabricating using conventional methods and equipment.Applications:Medical equipment housingsElectrical equipment housingsInformation provided by Kydex, LLC.
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
Mechanical Properties Metric English Comments
Tensile Strength 50.9 MPa
7380 psi
ASTM D638
Flexural Strength 74.11 MPa
10750 psi
ASTM D790
Flexural Modulus 2.385 GPa
345.9 ksi
ASTM D790
Izod Impact, Notched 1.81 J/cm
3.39 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 73.3 °C
164 °F
unannealed; ASTM D648
82.7 °C
181 °F
annealed; ASTM D648
Flammability, UL94 V-0
V-0
5VA
5VA
Processing Properties Metric English Comments
Processing Temperature 163 - 204 °C
325 - 399 °F
Thermoforming
Descriptive Properties Value Comments
Ball Pressure Test Pass
IEC 60695-10-2