Axiall 3014 Rigid PVC, Extrusion

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 3014 Rigid PVC, Extrusion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 3014 is a base for use of wood flour up to 40 percent. Impact Strength & ToughnessFlame RetardantChemical ResistanceDimensional StabilityInformation provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 78
78
ASTM D-2240
Tensile Strength, Yield 48.3 MPa
7000 psi
ASTM D-638
Tensile Modulus 2.62 GPa
380 ksi
ASTM D-638
Flexural Strength 82.7 MPa
12000 psi
ASTM D-790
Flexural Modulus 3.10 GPa
450 ksi
ASTM D-790
Izod Impact, Notched 0.641 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.20 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Thermal Properties Metric English Comments
CTE, linear 122 µm/m-°C

@Temperature 20.0 °C
68.0 µin/in-°F

@Temperature 68.0 °F
ASTM D-696
Deflection Temperature at 1.8 MPa (264 psi) 65.6 °C
150 °F
ASTM D-648
Processing Properties Metric English Comments
Processing Temperature 163 - 168 °C
325 - 335 °F
Die Temperature 168 - 182 °C
335 - 360 °F
Melt Temperature 185 - 193 °C
365 - 380 °F
Descriptive Properties Value Comments
Cell Classification 1200433
ASTM D-4216
12444
ASTM D-1784