Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 182 - 204 °C | 360 - 399 °F | |
DSM Biomedical PurSil® AL 5 Aliphatic Thermoplastic Silicone Polyether Urethane
(discontinued **) PurSil® AL is a family of aliphatic, thermoplastic silicone polyether urethane copolymers. These polymers are formed by the incorporation of silicone in the polymer backbone together with polyether.. |
|||
Processing Temperature | 171 - 204 °C | 340 - 399 °F | Blow Molding Stock |
Chevron Phillips Marlex® HHM 5502-04BN HDPE Hexene Copolymer
(discontinued **) This resin allows the blow molder to reduce inventory of resin types, because it can be used to package bleach and most detergents. Meets ASTM D4976 - PE 235. ASTM D1248 - Type III, Class A, Cat.. |
|||
Processing Temperature | 121 - 204 °C | 250 - 399 °F | Average value: 163 °C Grade Count:12 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |
|||
Processing Temperature | 160 - 204 °C | 320 - 399 °F | Injection |
Dyna-Purge® V Purging Compound Designed for Purging Flexible and Rigid PVCGeneral Description:DYNA-PURGE V is a non-abrasive, non-chemical “engineered†thermoplastic purging compound, formulated to flow naturally throug.. |
|||
Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
DuPont Elvax® 260 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
DuPont Elvax® 265 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
DuPont Elvax® 450 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
DuPont Elvax® 460 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
DuPont Elvax® 660 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
DuPont Elvax® 670 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
DuPont Elvax® 360 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
DuPont Elvax® 550 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
DuPont Elvax® 560 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-003 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-005 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-046 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-050 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-051 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-072 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-081 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-082 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 182 - 204 °C | 360 - 399 °F | Optimum Extrusion Conditions |
DSM Biomedical PurSil® 35 Thermoplastic Silicone Polyether Polyurethane (TSPU) A novel copolymer that is strong yet flexible with proven biocompatibility and biostability
Combining the benefits of both silicone elastomers and polyether urethanes, PurSil® TSPU has exceptional.. |
|||
Processing Temperature | 93.0 - 204 °C | 199 - 399 °F | |
DuPont Teijin Films Mylar® 854 Polyester Packaging Film, 60 Gauge Data provided by DuPont Packaging Polymers.DuPont Melinex® DuPont Melinex® 854 is a clear, one side coextruded heat sealable surface similar to Melinex® 850. The opposite surface is adhesion pret.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-089 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-091 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-214 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 171 - 204 °C | 340 - 399 °F | Blow Molding |
Chevron Phillips Marlex® HHM 5202-02 BN High Density Ethylene Hexene-1 Copolymer High Density Ethylene Hexene-1 CopolymerCustomer Benefits: For the blow molder who wants to stock one resin that will be suitable for most of his customers' packaging needs. Lightweight containers .. |
|||
Processing Temperature | 171 - 204 °C | 340 - 399 °F | Blow Molding |
Chevron Phillips Marlex® HHM 5502 LD High Density Ethylene Hexene Copolymer with Antistat High Density Ethylene Hexene Copolymer with AntistatCustomer Benefits: This resin allows the blow molder to reduce inventory of resin types, because it can be used to package a wide range of product.. |
|||
Processing Temperature | 163 - 204 °C | 325 - 400 °F | Extrusion Temperature |
CPT C-Flex® R70-251 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Processing Temperature | 121 - 204 °C | 250 - 399 °F | |
DuPont Elvax® 250 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |