Kleerdex Kydex® 130 Acrylic/PVC Thermoplastic Sheet  (discontinued **)

Category Polymer , Thermoplastic , Acrylic (PMMA) , Vinyl (PVC) , PVC/Acrylic Alloy
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kleerdex Kydex® 130 Acrylic/PVC Thermoplastic Sheet  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Decorative thermoplastic sheetApplications: Appliances, laminations, electronics, in-store displays, medical devices, equipment housings, dental equipmentFeatures: For deep to hard to form parts or where good finished detail is required. Kydex 130 is more rigid than most other thermoplastics resulting in parts that are stiffer and that will deform less when loaded. Kydex meets the highest standards for chemical resistance. Kydex 130 is recognized by Underwriter's Laboratories for Std 94 V-0 and 5V in all gauges. It meets FAR 25.853(a) vertical burn requirements for use in aircrafts as thermoformed parts. For building products it Surface Burning Characteristics meets Class I/A requirements. Fabrication: Kydex 130 is easy to fabricate and thermoform and since the color is integral throughout the sheet you don't have to worry about the cap thinning out or the substrate bleeding through.Data provided by the Kleerdex Company.Kleerdex Company became KYDEX, LLC in 2009.
Physical Properties Metric English Comments
Density 1.33 - 1.37 g/cc
0.0480 - 0.0495 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell R 101
101
ASTM D785
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ASTM D638
Elongation at Break 130 %
130 %
Modulus of Elasticity 2.372 GPa
344.0 ksi
Flexural Yield Strength 62.0 MPa
8990 psi
ASTM D790
Izod Impact, Notched 1.87 J/cm

@Temperature 23.0 °C
3.50 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 77.0 °C
171 °F
annealed; ASTM D648
Flammability, UL94 V-0
V-0
V-0, 5V; UL Standard 94
Processing Properties Metric English Comments
Processing Temperature 163 - 200 °C
325 - 392 °F
Forming Temperature