Processing Properties Metric English Comments
Processing Temperature 168 - 174 °C
335 - 345 °F
Suggested Stock
S&E Specialty Polymers TufTech™ GA-96-120 PVC Compound
Application: A Flame Retardant Wire & Cable Jacketing Compound Rated at 75°C With Superior Low Temperature Properties and UV Resistance.Information provided by S&E Specialty Polymers
Processing Temperature 163 - 174 °C
325 - 345 °F
Recommended Stock Temperature
Sylvin Technologies 5132-75 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.
Processing Temperature 163 - 174 °C
325 - 345 °F
Recommended Stock Temperature
Sylvin Technologies 5123 PVC Wire/Cable Compound
Information provided by Sylvin Technologies Inc.