Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 50.0 °C | 122 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 46-10/03 Polyester based TPU
(discontinued **) TPUs for Solvent-based adhesivesApplications: Others, FurnitureInformation provided by Merquinsa |
|||
Processing Temperature | >= 50.0 °C | >= 122 °F | Activation Temperature; EN-12961 |
Lubrizol Advanced Materials Pearlstick® 46-10/01 Linear Thermoplastic Polyurethane Elastomer Pearlstick 46-10/01 is an elastic, linear, aromatic polyurethane with a very high crystallization rate and a very high thermoplasticity level, available as pellets.Solubility: Pearlstick 46-10/.. |
|||
Processing Temperature | 50.0 °C | 122 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 45-60/08 Polycaprolactone based TPU Pearlstick 45-60/14 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a medium thermoplasticity level. Sol.. |
|||
Processing Temperature | 50.0 °C | 122 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 45-60/18 Polycaprolactone based TPU Pearlstick 45-60/18 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization speed and a low thermoplasticity level. Solub.. |
|||
Processing Temperature | 50.0 °C | 122 °F | hopper drying (4h) |
Borealis Supersmooth™ LE0592S Polyethylene Supersmooth™ LE0592S is a crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. Supersmooth™ LE0592S is intended for semiconductive applicat.. |
|||
Processing Temperature | 50.0 - 60.0 °C | 122 - 140 °F | Tacking Temperature |
Aquabond Technologies Aquabond™ ABS-85 Water Soluble Adhesive and Bonding Thermoplastic Description: Aquabond's water soluble thermoplastic is designed for temporary mounting of hard materials for slicing, dicing, grinding, lapping and polishing and comes in 3 different bonding tem.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Aremco-Seal™ 617 High Temperature Glass Coating Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1500 ºF (816 ºC). |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 552 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 618-N High Temperature Ceramic Adhesive/Paste, Silica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 632 High Temperature Ceramic Adhesive/Paste, Mica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 670 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 671 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 685-N High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 835 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 885 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco HiE-Coat™ 840-C High Emissivity Coating, Inorganic-Ceramic Filled Ceramic-based, black-pigmented coating for ceramic fiber modules and refactories to 2500°F (1371°C) |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco HiE-Coat™ 840-CM High Emissivity Coating, Inorganic-Ceramic Filled Ceramic-based, black-pigmented coating for dense refractories to 2500°F (1371°C) and stainless steel to 900°F (482°C) |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco HiE-Coat™ 840-M High Emissivity Coating, Inorganic-Ceramic Filled Ceramic-based, black-pigmented coating for carbon and stainless steel to 2000 °F (1093°C). |
|||
Processing Temperature | 50.0 - 120 °C | 122 - 248 °F | Application Temp |
Aremco HiE-Coat™ 840-MS High Emissivity Silicone-Ceramic Coating 840-C is a silicone-ceramic, black-pigmented coating for aluminum, brass, copper, and carbon and stainless steels to 1100 ºF (593 ºC).The HiE-Coat™ line of high emissivity coatings are black-body.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Pyro-Paint™ 634-ALP High Temperature Refractory Coating This phosphate-bonded, alumina coating system bonds exceptionally well to dense refractory ceramics, providing high abrasion and corrosion resistance for operating temperatures to 3200°F (1760°C) |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application |
Aremco Ceramabond™ 503 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 569 High Temperature Ceramic Adhesive/Paste, Alumina Filled White paste used for bonding of Ceramic-to-Ceramic; Ceramic-Metal; and Quartz. Used in Heaters, Igniters, Resistors, Sensors. This one component system air dries in 1-2 hrs and is ready for use fol.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 835-M High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 865 High Temperature Ceramic Adhesive/Paste, Aluminum Nitride Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 890 High Temperature Ceramic Adhesive/Paste, Silicon Carbide Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramacoat™ 512-N High Temperature Potting & Casting Material Silica Viscous, off-white paste for circuit breakers, power resistors and solenoids to 240°F (1316°C) |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 °C | 122 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 45-60/25 Polycaprolactone based TPU Pearlstick 45-60/25 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with an extremely high crystallization rate and a low thermoplasticity level. Solubili.. |
|||
Processing Temperature | 50.0 °C | 122 °F | Min. Activation Temp; EN 12961 |
Lubrizol Advanced Materials Pearlstick® 46-10/06 Polyester based TPU Pearlstick® 46-10/06 is an elastic, linear, aromatic polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a high thermoplasticity level. Solubility: .. |