Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 80.0 - 90.0 °C @Time 1800 sec |
176 - 194 °F @Time 0.500 hour |
|
Henkel Turco Scale Gon 5 Jet Engine Cleaner Turco Scale Gon 5 is an acid-activated, yellow liquid used in the Turco Jet Engine Process to condition and remove high temperature scale from jet engine parts. Approved by Rolls-Royce, GEAE and Pra.. |
|||
Processing Temperature | 80.0 - 90.0 °C @Time 1800 sec |
176 - 194 °F @Time 0.500 hour |
|
Henkel Turco Scale Gon 7 Jet Engine Cleaner Turco Scale Gon 7 is an acid-activated, yellow liquid used in the Turco Jet Engine Process to condition and remove high temperature scale from jet engine parts. Approved by Rolls-Royce.Application: .. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Aremco-Seal™ 613 High Temperature Glass Coating Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1150 ºF (620 ºC) |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 552 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 571 High Temperature Ceramic Adhesive/Paste, Magnesium Oxide Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled Aremco Ceramabond™ 600-N High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 618-N High Temperature Ceramic Adhesive/Paste, Silica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 632 High Temperature Ceramic Adhesive/Paste, Mica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 670 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 671 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 685-N High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 835-MB High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 885 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 40.0 - 90.0 °C | 104 - 194 °F | Application Temp |
Aremco Graphi-Bond™ 551-RN High Temperature Ceramic Adhesive/Paste, Graphite Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco HiE-Coat™ 840-CM High Emissivity Coating, Inorganic-Ceramic Filled Ceramic-based, black-pigmented coating for dense refractories to 2500°F (1371°C) and stainless steel to 900°F (482°C) |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Pyro-Paint™ 634-ALP High Temperature Refractory Coating This phosphate-bonded, alumina coating system bonds exceptionally well to dense refractory ceramics, providing high abrasion and corrosion resistance for operating temperatures to 3200°F (1760°C) |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application |
Aremco Ceramabond™ 503 High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 569 High Temperature Ceramic Adhesive/Paste, Alumina Filled White paste used for bonding of Ceramic-to-Ceramic; Ceramic-Metal; and Quartz. Used in Heaters, Igniters, Resistors, Sensors. This one component system air dries in 1-2 hrs and is ready for use fol.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 668 High Temperature Ceramic Adhesive/Paste, Alumino-Silica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 835-M High Temperature Ceramic Adhesive/Paste, Alumina Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 865 High Temperature Ceramic Adhesive/Paste, Aluminum Nitride Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramabond™ 890 High Temperature Ceramic Adhesive/Paste, Silicon Carbide Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Ceramacoat™ 512-N High Temperature Potting & Casting Material Silica Viscous, off-white paste for circuit breakers, power resistors and solenoids to 240°F (1316°C) |
|||
Processing Temperature | 50.0 - 90.0 °C | 122 - 194 °F | Application Temp |
Aremco Graphi-Bond™ 669 High Temperature Ceramic Adhesive/Paste, Graphite Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |