Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol Advanced Materials Pearlstick® 46-10/01 Linear Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlstick®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials Pearlstick® 46-10/01 Linear Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Pearlstick 46-10/01 is an elastic, linear, aromatic polyurethane with a very high crystallization rate and a very high thermoplasticity level, available as pellets.Solubility: Pearlstick 46-10/01 is soluble in methylene chloride, acetone, methyl ethyl ketone (MEK), ethyl acetate and tetrahydrofuran (THF). Diluting solvents such as toluene can be added in large amounts.The solvents and diluents should be water-free (max 0.1%), so as to avoid subsequent side reactions during crosslinking with isocyanates.Solutions: Pearlstick 46-10/01 should be dissolved in closed tanks, and the use of a variable speed agitator is advised. The final viscosity fies can vary, depending on the stirring process and on the solvent/diluents ratios.Applications: Pearlstick 46-10/01 is used for the production of adhesives for bonding plasticized PVC to plasticized PVC or other materials such as leather, textiles, metals, paper, etc.Pearlstick 46-10/01 enables the production of adhesives with high solids content and low viscosity, which are adequate for application in the wood and shoe industries. The addition of a poly-functional isocyanate improves the heat-resistance and the strength of the joints.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
ISO 2781
Brookfield Viscosity 100 - 200 cP

@Temperature 20.0 °C
100 - 200 cP

@Temperature 68.0 °F
Brookfield RVF sp. 2, 20 rpm solution at 15% in MEK; MQSA N0 40A
Processing Properties Metric English Comments
Processing Temperature >= 50.0 °C
>= 122 °F
Activation Temperature; EN-12961
Descriptive Properties Value Comments
Color white or slightly yellowish
Crystallization Rate Very High
Hydroxyl Content Approx. 0.1%
MQSA 47A
Thermoplasticity Range Very High