Material Notes:
Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and do not outgas after curing. They are also environmentally safe, non-flammable materials which contain no volatile organic compounds.General Features: Ceramic Fiber-Reinforced Bonding: Graphite, Carbon Principal Use: Structures, Molds
Physical Properties Metric English Comments
Density 1.45 - 1.50 g/cc
0.0524 - 0.0542 lb/in³
Volatile Organic Compounds (VOC) Content 0.000 g/l
0.000 g/l
Viscosity 20000 - 40000 cP
20000 - 40000 cP
Mechanical Properties Metric English Comments
Impact Test 35.3 J
26.0 ft-lb
Torque Strength; curing at 1000°F
Thermal Properties Metric English Comments
CTE, linear 7.56 µm/m-°C
4.20 µin/in-°F
Maximum Service Temperature, Air 760 °C
1400 °F
Electrical Properties Metric English Comments
Dielectric Strength 4.13 kV/mm
105 kV/in
Processing Properties Metric English Comments
Processing Temperature 50.0 - 90.0 °C
122 - 194 °F
Application Temp
Cure Time 120 min

@Temperature 93.3 °C
2.00 hour

@Temperature 200 °F
preceeded by 1-4 hour air set
Shelf Life 6.00 Month

@Temperature 4.44 - 32.2 °C
6.00 Month

@Temperature 40.0 - 90.0 °F
Descriptive Properties Value Comments
Acid Resistance Good
after curing at 700°F for 2 hours
Alkali Resistance Good
after curing at 700°F for 2 hours
Color Black
Moisture Resistance Excellent
after curing at 700°F for 2 hours
Solvent Water
Thinner 669-T