Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Celcon® M90AW POM, Tribological
(Unverified Data**) Celcon® M90AW is a low wear grade designed for gears and other low wear applications, especially where reducing noise and wear in low load-high velocity applications. Celcon® M90AW is an option .. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Celcon® MC270 POM, Mineral Reinforced
(Unverified Data**) Celcon® MC270 is a mineral coupled acetal copolymer designed for applications requiring improved stiffness, lower mold shrinkage and reduced warpage while maintaining the mechanical performance cha.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Celcon® MC90-HM POM, Mineral Reinforced
(Unverified Data**) Celcon® MC90-HM is a highly mineral filled and coupled M90 material for producing very flat and dimensionally stable parts (normal flow).Mineral coupled for reduced warpage, high modulus, moderate .. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Hostaform® C 27021 POM
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMInjection molding grade with high flowInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Hostaform® C 9021 TF5 POM, Tribological
(Unverified Data**) Hostaform® C 9021 TF5 is a standard flow low level polytetraflouroethylene filled (PTFE) product designed for use in wear applications against plastics, metal, glass or ceramic mating surfaces whe.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese ZENITE 5130L LCP, 30% Glass Reinforced
(Unverified Data**) Zenite 5130L is a 30% glass-reinforced LCP resin with improved toughness30% glass-reinforced, lubricatedInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese ZENITE 7130 LCP, 30% Glass Reinforced
(Unverified Data**) Zenite® 7130 is a 30% glass fiber reinforced liquid crystal polymer for injection molding. It has excellent impact resistance and excellent heat deflection temperature.30% glass reinforced, excelle.. |
|||
Processing Temperature | 90.0 - 120 °C | 194 - 248 °F | cavity |
Celanese Celcon® GC15 POM, 15% Glass Reinforced Celcon« GC15 is an acetal copolymer grade utilizing a nominal 15 wt. % fiber glass level to increase stiffness and strength.Information provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Celcon® M90-45XAP® POM, Specialty Celcon« acetal copolymer grade M90-45XAP« is a UV resistant, low emission version, medium viscosity polymer providing optimum performance in general purpose injection molding primarily for the in.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Celcon® MR50B POM, Specialty Celcon« MR50B is a specialty media resistant grade developed for improved bleach resistance and improved toughness.Information provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Hostaform® C 9021 SW XAP² ™ LS POM, Tribological POM copolymerInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Hostaform® M90XAP® POM, Unfilled Hostaform« acetal copolymer grade M90 XAP« is a low emission version, medium viscosity polymer providing optimum performance in general purpose injection molding primarily for the interior automo.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese VECTRA A150 LCP, 50% Glass Reinforced Improved creep resistance over A130. May reduce warpage in some parts compared to A130. 50% glass reinforced.50% glass fiber, improved creep resistance over A130A three-zone screw evenly divided int.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese VECTRA A435 LCP, 35% Specialty Best High Current Arc Ignition (HAI) performance. Glass/PTFE filled.Information provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese VECTRA A625 LCP, 25% Specialty Good wear characteristics. 25% graphite filled.Information provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese VECTRA E440i LCP, 42% Mineral / Glass Reinforced Mineral and glass filled grade with low warp, easy flow and smooth surface apperance.Information provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese VECTRA E471i LCP, 35% Specialty Low warp with excellent propertiesInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese VECTRA MT1300 LCP, Medical Technology Unreinforced Vectra grade suitable for extrusion.Information provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese ZENITE 6330L LCP, 30% Mineral Reinforced Zenite 6330L is a lubricated 30% mineral-reinforced LCP resin having excellent toughness. It is well suited for use in the automotive, electrical/electronic, telecommunications, and aerospace indus.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Celcon® CF802 POM, Specialty Celcon« acetal copolymer grade CF802 is a conductive, fuel compatible general purpose acetal copolymer. Celcon« CF802 has been developed to dissipate static electricity from fuel handling systems... |
|||
Processing Temperature | 90.0 - 120 °C | 194 - 248 °F | Cavity temperature |
Celanese Celstran® PA66-GF50-0111P7.5/11 PA666, 50% Glass Reinforced Material code according to ISO 1043-1: PA66PA66/6 copolymer with 50% ash content - 7.5mmInformation provided by Celanese |
|||
Processing Temperature | 90.0 - 120 °C | 194 - 248 °F | Cavity temperature |
Celanese Celcon® GC10 POM, 10% Glass Reinforced
(Unverified Data**) Celcon® GC10 acetal copolymer is a 10% glass reinforced acetal for improved strength and stiffness.10% glass fiber, has been replaced with Hostaform® C 9021 GV1/10Standard reciprocating screw inje.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Celcon® MC270-HM POM, Mineral Reinforced
(Unverified Data**) Celcon® MC270-HM is a high modulus, mineral coupled acetal copolymer. It utilizes a higher additive level to provide significant improvement in product stiffness and mold shrinkage and better warp.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Hostaform® C 9021 AW POM, Tribological
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMInjection molding type like C 9021, with special additive modifiedInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Hostaform® C 9021 TF POM, Tribological
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMInjection molding type like C 9021, with PTFE modifiedInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Hostaform® C 9021 GV3/10 POM, 10% Glass Reinforced Chemical abbreviation according to ISO 1043-1: POMInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Hostaform® CF802 10/9022 POM, Specialty Hostaform« acetal copolymer grade CF802 10/9022 is a conductive, fuel compatible general purpose acetal copolymer. Hostaform« CF802 10/9022 has been developed to dissipate static electricity from .. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Hostaform® MT® SlideX™ 2404 POM, Medical Technology POM copolymerInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese VECTRA MT1305 LCP, 15% Glass Reinforced Provides easier flow than MT1310. Slightly tougher, but may warp slightly more than MT1310 in some parts. 15% glass reinforced.Information provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Celcon® MR270B POM, Specialty Celcon« MR270B is a high flow specialty media resistant grade developed for improved bleach resistance.Information provided by Celanese |