Processing Properties | Metric | English | Comments |
---|---|---|---|
Processing Temperature | 90.0 - 120 °C | 194 - 248 °F | Cavity temperature |
Celanese Celcon® GC25A POM, 25% Glass Reinforced
(Unverified Data**) Celcon® acetal copolymer grade GC25A is a glass coupled formulation containing 25% reinforced fiber glass. This grade offers excellent strength, stiffness and heat distortion temperature with lower.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Celcon® M25UV POM, UV Resistant
(Unverified Data**) Celcon® M25UV is an acetal copolymer developed as a natural UV light stabilized low flow, high molecular weight grade. It has been formulated as a natural acetal that does not discolor, yet maintai.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Celcon® M90™ POM
(Unverified Data**) Celcon acetal copolymer grade M90™ is a medium viscosity polymer providing optimum performance in general purpose injection molding and extrusion of thin walled tubing and thin gauge film. This gr.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Hostaform® C 27021 GV3/30 POM, 30% Glass Reinforced
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMInjection molding grade with high flow, with 30 % glass spheres reinforcedInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Hostaform® C 9021 M POM, Tribological
(Unverified Data**) Chemical abbreviation according to ISO 1043-1: POMInjection molding type like C 9021, with molybdenum disulphide modifiedInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Hostaform® MT8U05 POM, Medical Technology
(Unverified Data**) Hostaform® acetal copolymer grade MT8U05 is a special grade developed for medical industry applications containing low residual monomers and no animal products. The material can be identified by U.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese ZENITE 7244 LCP, 40% Mineral / Glass Reinforced
(Unverified Data**) Zenite 7244 is a 40% glass mineral reinforced liquid crystal polymer resin with a high heat deflection temperature of 295C, high flow and good flatness."Information provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese ZENITE ZE55201 LCP, 50% Mineral / Glass Reinforced
(Unverified Data**) Zenite® ZE55201 is a 50% mineral/glass fiber reinforced liquid crystal polymer for injection molding. and It is specifically suitable for applications requiring ultra flatness.50% glass/mineral rei.. |
|||
Processing Temperature | 90.0 - 120 °C | 194 - 248 °F | Cavity temperature |
Celanese Celstran® PA66-GF50-0112P7,5/10 PA666, 50% Glass Reinforced
(Unverified Data**) Material code according to ISO 1043-1: PA66PA66/6 copolymer with 50% ash content high gloss, UV stabilized, UL - listing (f1)Information provided by Celanese |
|||
Processing Temperature | 100 - 120 °C | 212 - 248 °F | conductor preheating temperature |
Borealis Borcell™ ME1244 Medium Density Polyethylene Borcell™ ME1244 is a fully formulated compound for chemical foamed telesingles. ME1244 is a medium-density polyethylene compound containing chemical blowing agent. Applications Borcell™ ME1244 i.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Hostaform® C 9021 SW XAP² ™ LS POM, Tribological POM copolymerInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Hostaform® MR130ACS POM, Specialty Hostaform« acetal copolymer grade MR130ACS is a general purpose acetal with improved acid stabilization. Hostaform« MR130ACS demonstrates improved performance over standard acetals after intermit.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Hostaform® SlideX™ C0313 XAP² ™ POM, Tribological POM copolymerInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese THERMX CG923 PCT, 20% Glass Reinforced Thermx« CG923 is a 20% glass fiber reinforced and flame retardant polycyclohexylenedimethylene terephthalate for injection molding.Information provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese THERMX CG943 PCT, 40% Glass Reinforced Thermx« CG943 is a 40% glass fiber reinforced and flame retardant polycyclohexylenedimethylene terephthalate for injection molding.Information provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese VECTRA E471i LCP, 35% Specialty Low warp with excellent propertiesInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese ZENITE 7244 LCP, 40% Mineral / Glass Reinforced Zenite 7244 is a 40% glasslmineral reinforced liquid crystal polymer resin with a high heat deflection temperature of 295C, high flow and good flatness."Information provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Celcon® M90™ POM, Unfilled Celcon acetal copolymer grade M90Ö is a medium viscosity polymer providing optimum performance in general purpose injection molding and extrusion of thin walled tubing and thin gauge film. This gr.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Celcon® MR25B POM, Specialty Celcon« MR25B is a specialty media resistant grade developed for improved bleach resistance and improved toughness.Information provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Celcon® MR90B POM, Specialty Celcon« MR90B is a standard flow specialty media resistant grade developed for improved bleach resistance.Information provided by Celanese |
|||
Processing Temperature | 90.0 - 120 °C | 194 - 248 °F | cavity |
Celanese Celstran® PA66-GF50-02 P7/12 Nylon 66, 50% Glass Reinforced Material code according to ISO 1043-1: PA66Information provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese THERMX CG933 PCT, 30% Glass Reinforced Thermx« CG933 is a 30% glass fiber reinforced and flame retardant polycyclohexylenedimethylene terephthalate for injection molding.Information provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese VECTRA A530 LCP, 30% Mineral Reinforced Best overall surface appearance with properties similar to A130. Less abrasive than glass fiber reinforced grades. Improved toughness over A130. Outstanding hydrolytic stability. Recommended wher.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Hostaform® M90XAP® POM
(Unverified Data**) Hostaform® acetal copolymer grade M90 XAP® is a low emission version, medium viscosity polymer providing optimum performance in general purpose injection molding primarily for the interior automo.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Hostaform® S 9362 POM, Impact Modified
(Unverified Data**) Hostaform® acetal copolymer grade S 9362 is an impact modified grade for applications requiring improved impact. Hostaform® S 9362 provides good impact strength while improving modulus and weld .. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Celcon® LW90-F2 POM, Tribological Celcon« LW90-F2 is an acetal copolymer formulated with a nominal 9 melt flow rate base polymer and a standard level of polytetrafluoroethylene filler (PTFE). It is designed for use in wear applicat.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Hostaform® C 9021 XAP® POM, Unfilled POM copolymerInformation provided by Celanese |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | Cavity temperature |
Celanese Thermx® CG943 PCT, 40% Glass Reinforced
(Unverified Data**) Thermx® CG943 is a 40% glass fiber reinforced and flame retardant polycyclohexylenedimethylene terephthalate for injection molding.40% glass reinforced, flame retardantInformation provided by Celan.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese Celcon® MC270-HM POM, Mineral Reinforced Celcon« MC270-HM is a high modulus, mineral coupled acetal copolymer. It utilizes a higher additive level to provide significant improvement in product stiffness and mold shrinkage and better warp.. |
|||
Processing Temperature | 80.0 - 120 °C | 176 - 248 °F | cavity |
Celanese VECTRA C130 LCP, 30% Glass Reinforced Has the same excellent balance of properties as A130 with higher temperature capability and easier flow. Slightly more dimensional stability in vapor phase soldering than A130. Suitable for some i.. |