Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 54.0 - 160 µm/m-°C | 30.0 - 88.9 µin/in-°F | Average value: 105 µm/m-°C Grade Count:7 |
Overview of materials for Thermoset Polyurethane, Liquid This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear | 130 - 160 µm/m-°C @Temperature 20.0 °C |
72.2 - 88.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Solef® 1015/0078 PVDF Homopolymer
(discontinued **) Key features of this grade: Plasticized, Offshore, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorina.. |
|||
CTE, linear | 130 - 160 µm/m-°C @Temperature 20.0 °C |
72.2 - 88.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer
(discontinued **) Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i.. |
|||
CTE, linear | 65.0 - 160 µm/m-°C | 36.1 - 88.9 µin/in-°F | Average value: 121 µm/m-°C Grade Count:12 |
Overview of materials for Polytetrafluoroethylene (PTFE), Conductive Carbon Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Conductive Carbon Filled". Each property range of values reported is min.. |
|||
CTE, linear | 72.0 - 160 µm/m-°C | 40.0 - 88.9 µin/in-°F | Average value: 88.1 µm/m-°C Grade Count:26 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
CTE, linear | 140 - 160 µm/m-°C @Temperature 20.0 °C |
77.8 - 88.9 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer
(discontinued **) Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD.. |