Hippe PE 300 Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Erhard Hippe KG
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hippe PE 300 Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologically safe. Low water absorption, not aromatic-resistant. Manifold usable. Easily machinable. Excellent sliding properties. The abrasion is very low.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 0.950 - 0.960 g/cc
0.950 - 0.960 g/cc
DIN 53 479
Moisture Absorption at Equilibrium <= 0.050 %
<= 0.050 %
Absorption of humidity in standard operating environment; DIN 53 715
Water Absorption at Saturation <= 0.050 %
<= 0.050 %
DIN 53 495
Mechanical Properties Metric English Comments
Ball Indentation Hardness 54.0 - 60.0 MPa

@Time 30.0 sec
7830 - 8700 psi

@Time 0.00833 hour
DIN 53 456
Tensile Strength 24.0 - 31.0 MPa
3480 - 4500 psi
DIN 53 455
Elongation at Break 400 - 800 %
400 - 800 %
DIN 53 455
Tensile Modulus 1.00 - 1.40 GPa
145 - 203 ksi
DIN 53 457
Flexural Modulus 1.00 - 1.40 GPa
145 - 203 ksi
from bending test; DIN 53 457
Charpy Impact, Notched NB
NB
DIN 53 453
Coefficient of Friction, Dynamic 0.29
0.29
Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Tear Strength Test 36
36
in MPa; DIN 53 455
Abrasion 1.0
1.0
µm/km; Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Thermal Properties Metric English Comments
CTE, linear 130 - 150 µm/m-°C
72.2 - 83.3 µin/in-°F
Specific Heat Capacity 1.70 - 2.00 J/g-°C
0.406 - 0.478 BTU/lb-°F
Thermal Conductivity 0.350 - 0.430 W/m-K
2.43 - 2.98 BTU-in/hr-ft²-°F
Melting Point 128 - 133 °C
262 - 271 °F
DIN 53 736
Maximum Service Temperature, Air 90.0 °C
194 °F
Continuous use
120 °C
248 °F
Short Periods
Deflection Temperature at 0.46 MPa (66 psi) 70.0 - 85.0 °C
158 - 185 °F
ISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 42.0 - 49.0 °C
108 - 120 °F
ISO-R 75 Method A
Glass Transition Temp, Tg -95.0 °C
-139 °F
dynamic; DIN 53 736
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+16 ohm-cm
>= 1.00e+16 ohm-cm
DIN 53 482, VDE 0303, Part 3
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
DIN 53 482
Dielectric Constant 2.4

@Frequency 1.00e+6 Hz
2.4

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength 150 kV/mm
3810 kV/in
Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index 0.00020

@Frequency 1.00e+6 Hz
0.00020

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Descriptive Properties Value Comments
Color natural/black
Creep Resistance Grade KA 3c
DIN 53 480, IEC-112, VDE 0303 Part 1
Resistance to hot water, suds resistant