Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Micropol Isoplas P471 Crosslinkable Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Micropol Limited
Trade Name Isoplas
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Micropol Isoplas P471 Crosslinkable Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Micropol Limited
Physical Properties Metric English Comments
Density 0.947 g/cc
0.0342 lb/in³
ASTM D792
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.0 MPa
3480 psi
ASTM D638
Elongation at Break 200 %
200 %
Modulus of Elasticity 0.780 GPa

@Temperature 20.0 °C
113 ksi

@Temperature 68.0 °F
Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C

@Temperature 20.0 °C
72.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 2.00 J/g-°C
0.478 BTU/lb-°F
Thermal Conductivity 0.431 W/m-K
2.99 BTU-in/hr-ft²-°F
Vicat Softening Point 120 °C
248 °F
ASTM D1525