Fluoropolymer material specifications.Information provided by Isoflon.
Physical Properties Metric English Comments
Specific Gravity 1.70 - 1.75 g/cc
1.70 - 1.75 g/cc
ISO 12086
Water Absorption 0.020 %
0.020 %
DIN 53 495
Mechanical Properties Metric English Comments
Hardness, Shore D 62 - 72
62 - 72
DIN 53 505
Ball Indentation Hardness 34.0 - 40.0 MPa
4930 - 5800 psi
DIN 53 456
Tensile Strength 36.0 - 48.0 MPa
5220 - 6960 psi
DIN 53455
Elongation at Break 200 - 350 %
200 - 350 %
DIN 53455
Tensile Modulus 0.500 - 1.20 GPa
72.5 - 174 ksi
DIN 53457
Coefficient of Friction, Dynamic 0.40
0.40
on steel
Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C

@Temperature 20.0 - 100 °C
72.2 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 0.170 W/m-K
1.18 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 150 °C
302 °F
Continuous
Minimum Service Temperature, Air -100 °C
-148 °F
Continuous
Electrical Properties Metric English Comments
Dielectric Strength 60.0 - 90.0 kV/mm
1520 - 2290 kV/in
DIN 53481