Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 88.9 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 54.0 - 160 µm/m-°C
30.0 - 88.9 µin/in-°F
Average value: 105 µm/m-°C Grade Count:7
Overview of materials for Thermoset Polyurethane, Liquid
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of..
CTE, linear 130 - 160 µm/m-°C

@Temperature 20.0 °C
72.2 - 88.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Solvay Specialty Polymers Solef® 1015/0078 PVDF Homopolymer  (discontinued **)
Key features of this grade: Plasticized, Offshore, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorina..
CTE, linear 130 - 160 µm/m-°C

@Temperature 20.0 °C
72.2 - 88.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Solvay Specialty Polymers Solef® 61010 PVDF Copolymer  (discontinued **)
Key features of this grade: Permanent Plasticizing, Fuel Line, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF i..
CTE, linear 65.0 - 160 µm/m-°C
36.1 - 88.9 µin/in-°F
Average value: 121 µm/m-°C Grade Count:12
Overview of materials for Polytetrafluoroethylene (PTFE), Conductive Carbon Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Conductive Carbon Filled". Each property range of values reported is min..
CTE, linear 72.0 - 160 µm/m-°C
40.0 - 88.9 µin/in-°F
Average value: 88.1 µm/m-°C Grade Count:26
Overview of materials for Nylon 46, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
CTE, linear 140 - 160 µm/m-°C

@Temperature 20.0 °C
77.8 - 88.9 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Solvay Specialty Polymers Solef® 11008 PVDF Copolymer  (discontinued **)
Key features of this grade: Low Viscosity, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVD..
Copyright © lookpolymers.com All Rights Reserved