Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 4.70 - 150 µm/m-°C | 2.61 - 83.3 µin/in-°F | Average value: 51.6 µm/m-°C Grade Count:29 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
CTE, linear | 30.0 - 150 µm/m-°C | 16.7 - 83.3 µin/in-°F | Average value: 70.2 µm/m-°C Grade Count:168 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
CTE, linear | 130 - 150 µm/m-°C @Temperature 20.0 °C |
72.2 - 83.3 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Solef® 31008 PVDF Copolymer
(discontinued **) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
CTE, linear | 130 - 150 µm/m-°C @Temperature 20.0 °C |
72.2 - 83.3 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Solvay Specialty Polymers Solef® 32008 PVDF Copolymer
(Unverified Data**) Key features of this grade: High Flexibility/ High Elongation/Cold Impact Resistance, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General .. |
|||
CTE, linear | 75.0 - 150 µm/m-°C | 41.7 - 83.3 µin/in-°F | Average value: 108 µm/m-°C Grade Count:3 |
Overview of materials for Polytetrafluoroethylene (PTFE), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Carbon Fiber Filled". Each property range of values reported is minimum .. |
|||
CTE, linear | 90.0 - 150 µm/m-°C | 50.0 - 83.3 µin/in-°F | Average value: 113 µm/m-°C Grade Count:7 |
Overview of materials for Nylon 11, Flexible Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11, Flexible Tubing Grade". Each property range of values reported is minimum and maximum values o.. |
|||
CTE, linear | 80.0 - 150 µm/m-°C | 44.4 - 83.3 µin/in-°F | Average value: 103 µm/m-°C Grade Count:3 |
Overview of materials for Nylon 12, Graphite Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Graphite Filled". Each property range of values reported is minimum and maximum values of appr.. |
|||
CTE, linear | 50.0 - 150 µm/m-°C | 27.8 - 83.3 µin/in-°F | Average value: 96.4 µm/m-°C Grade Count:20 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
CTE, linear | 100 - 150 µm/m-°C @Temperature 20.0 - 100 °C |
55.6 - 83.3 µin/in-°F @Temperature 68.0 - 212 °F |
DIN 53752 |
Schwartz Technical Plastics LAMIGAMID® 400 Cast Polyamide 6, Elastomer Modified, Dry Application: gear-wheels, chain-wheels, hydrocyclones, housings, outrigger floatsInformation provided by Schwartz Technical Plastics GmbH |
|||
CTE, linear | 130 - 150 µm/m-°C | 72.2 - 83.3 µin/in-°F | |
Hippe PE 300 Polyethylene Tough, flexible and stiff, depending on the crystalline structure (density). Resinous surface. Excellent dielectric properties, Good resistance against solvents, acids and alkalis. Physiologicall.. |
|||
CTE, linear | 7.20 - 150 µm/m-°C | 4.00 - 83.3 µin/in-°F | Average value: 48.9 µm/m-°C Grade Count:143 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |