Material Notes:
Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Moisture Absorption at Equilibrium 0.22 %
0.22 %
60% RH; ASTM D570
Linear Mold Shrinkage 0.020 cm/cm
0.020 in/in
ASTM D955
Melt Flow 27 g/10 min
27 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 80
80
ASTM D785
Tensile Strength 64.0 MPa
9280 psi
ASTM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Strength 93.0 MPa
13500 psi
ASTM D790
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Izod Impact, Notched 0.560 J/cm
1.05 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C
72.2 µin/in-°F
ASTM D696
Melting Point 166 °C
331 °F
ASTM D1525
Deflection Temperature at 0.46 MPa (66 psi) 158 °C
316 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
ASTM D648
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+10 ohm-cm
1.00e+10 ohm-cm
ASTM D257
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
ASTM D257
Dielectric Constant 3.7
3.7
ASTM D150
Dielectric Strength 19.0 kV/mm
483 kV/in
ASTM D149
Dissipation Factor 0.060

@Frequency 1.00e+6 Hz
0.060

@Frequency 1.00e+6 Hz
ASTM D150