Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers KetaSpire® KT-880P Polyetheretherketone (PEEK)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers KetaSpire® KT-880P Polyetheretherketone (PEEK)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KetaSpire KT-880P is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color coarse powder form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, ease of melt processing, high purity and excellent chemical resistance to organics, acids and bases. These properties make it well-suited for applications in healthcare, transportation, electronics, chemical processing and other industrial uses. KetaSpire KT-880P is intended for extrusion compounding. This powder is also available as KT-880NT in a natural-color pellet form for injection molding.Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Melt Flow 36 g/10 min

@Load 2.16 kg,
Temperature 400 °C
36 g/10 min

@Load 4.76 lb,
Temperature 752 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 100 MPa
14500 psi
ASTM D638
Elongation at Break 10 - 20 %
10 - 20 %
Crystallized; ASTM D638
>= 60 %
>= 60 %
Quenched; ASTM D638
Elongation at Yield 5.2 %
5.2 %
ASTM D638
Tensile Modulus 3.80 GPa
551 ksi
ASTM D638
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 3.90 GPa
566 ksi
ASTM D790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
NB
NB
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 50.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
27.8 µin/in-°F

@Temperature -58.0 - 122 °F
TMA; ASTM E831
Melting Point 343 °C
649 °F
ASTM D3417
Deflection Temperature at 1.8 MPa (264 psi) 159 °C
318 °F
Unannealed; ASTM D648
Glass Transition Temp, Tg 147 °C
297 °F
ASTM D3417
Descriptive Properties Value Comments
Appearance Natural Color
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Ductile
Fatigue Resistant
Flame Retardant
Good Chemical Resistance
Good Dimensional Stability
Good Impact Resistance
High Flow
High Heat Resistance
Forms Powder
Generic PEEK
Processing Method Compression Molding
Electrostatic Spray Coating
RoHS Compliance RoHS Compliant
Uses Electrical/Electronic Applications
Industrial Applications
Semiconductor Molding Compounds