Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)  (Unverified Data**)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent wear resistance, best-in-class fatigue resistance, ease of melt processing, high purity and excellent chemical resistance to organics, acids and bases. These properties make it well-suited for applications in healthcare, transportation, electronics, chemical processing and other industrial uses. KetaSpire KT-880 NT can be easily processed using typical injection molding processes. This resin is also available as KT-880P in a natural-color coarse powder form for compounding. Pellets of KT-880 are supplied lightly dusted with the lubricant calcium stearate (0.01% level) to aid with pellet conveyance in plastication screws. The equivalent unlubricated natural color grade of low flow KetaSpire is available as KT-880 NL. - Black: KT-880 BK 95 - Natural: KT-880 NTInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Viscosity 150000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
150000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt; ASTM D3835
Linear Mold Shrinkage, Flow 0.014 - 0.016 cm/cm

@Thickness 0.318 mm
0.014 - 0.016 in/in

@Thickness 0.0125 in
5" x 0.5" x 0.125"; ASTM D955
Linear Mold Shrinkage, Transverse 0.015 - 0.017 cm/cm

@Thickness 3.18 mm
0.015 - 0.017 in/in

@Thickness 0.125 in
5" x 0.5" x 0.125"; ASTM D955
Melt Flow 36 g/10 min

@Load 2.16 kg,
Temperature 400 °C
36 g/10 min

@Load 4.76 lb,
Temperature 752 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 102
102
M-Scale; ASTM D785
Tensile Strength 100 MPa
14500 psi
51 mm/min; ASTM D638
Tensile Strength, Yield 102 MPa
14800 psi
ISO 527-2/1A/50
Elongation at Break 10 - 20 %
10 - 20 %
50 mm/min; ASTM D638
10 - 20 %
10 - 20 %
ISO 527-2/1A/50
Elongation at Yield 5.0 %
5.0 %
ISO 527-2/1A/50
5.2 %
5.2 %
50 mm/min; ASTM D638
Tensile Modulus 3.70 GPa
537 ksi
1.0 mm/min; ASTM D638
4.00 GPa
580 ksi
ISO 527-2/1A/1
Flexural Strength 134 MPa
19400 psi
ISO 178
153 MPa
22200 psi
ASTM D790
Flexural Modulus 3.80 GPa
551 ksi
ASTM D790
3.90 GPa
566 ksi
ISO 178
Compressive Strength 123 MPa
17800 psi
ASTM D695
Poissons Ratio 0.37
0.37
ASTM E132
Shear Modulus 1.35 - 1.46 GPa
196 - 212 ksi
Calculated
Shear Strength 95.1 MPa
13800 psi
ASTM D732
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
NB
NB
ASTM D4812
Izod Impact, Notched (ISO) 4.90 kJ/m²
2.33 ft-lb/in²
ISO 180
Izod Impact, Unnotched (ISO) NB
NB
ISO 180
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 50.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
27.8 µin/in-°F

@Temperature -58.0 - 122 °F
TMA; ASTM E831
Specific Heat Capacity 1.33 J/g-°C

@Temperature 50.0 °C
0.318 BTU/lb-°F

@Temperature 122 °F
DSC
1.93 J/g-°C

@Temperature 200 °C
0.461 BTU/lb-°F

@Temperature 392 °F
DSC
Thermal Conductivity 0.250 W/m-K
1.74 BTU-in/hr-ft²-°F
ASTM E1530
Melting Point 343 °C
649 °F
Peak; ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
Annealed; ASTM D648
Glass Transition Temp, Tg 147 °C
297 °F
ASTM D3418
Electrical Properties Metric English Comments
Volume Resistivity 3.80e+17 ohm-cm
3.80e+17 ohm-cm
ASTM D257
Surface Resistance >= 1.90e+17 ohm
>= 1.90e+17 ohm
ASTM D257
Dielectric Constant 3.01

@Frequency 1000 Hz
3.01

@Frequency 1000 Hz
ASTM D150
3.07

@Frequency 1.00e+6 Hz
3.07

@Frequency 1.00e+6 Hz
ASTM D150
3.1

@Frequency 60.0 Hz
3.1

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm

@Thickness 3.00 mm
381 kV/in

@Thickness 0.118 in
ASTM D149
Dissipation Factor 0.0010

@Frequency 1000 Hz
0.0010

@Frequency 1000 Hz
ASTM D150
0.0010

@Frequency 60.0 Hz
0.0010

@Frequency 60.0 Hz
ASTM D150
0.0030

@Frequency 1.00e+6 Hz
0.0030

@Frequency 1.00e+6 Hz
ASTM D150
Processing Properties Metric English Comments
Rear Barrel Temperature 355 °C
671 °F
Middle Barrel Temperature 365 °C
689 °F
Front Barrel Temperature 370 °C
698 °F
Nozzle Temperature 375 °C
707 °F
Mold Temperature 175 - 205 °C
347 - 401 °F
Drying Temperature 150 °C
302 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Agency Ratings ISO 10993
ISO 10993-Part 1
Appearance Black
Natural Color
Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Features Autoclave Sterilizable
Biocompatible
Ductile
E-beam Sterilizable
Ethylene Oxide Sterilizable
Fatigue Resistant
Flame Retardant
Good Chemical Resistance
Good Dimensional Stability
Good Impact Resistance
Good Sterilizability
Heat Sterilizable
High Flow
High Heat Resistance
Radiation (Gamma) Resistant
Radiation Sterilizable
Radiotranslucent
Steam Resistant
Steam Sterilizable
Forms Pellets
Generic PEEK
Injection Rate Fast
Processing Method Extrusion Blow Molding
Fiber (Spinning) Extrusion
Film Extrusion
Injection Molding
Machining
Profile Extrusion
Thermoforming
Wire & Cable Extrusion
RoHS Compliance RoHS Compliant
Screw Compression Ratio 2.5:1.0 to 3.5:1.0
Uses Aircraft Applications
Connectors
Dental Applications
Electrical/Electronic Applications
Film
Hospital Goods
Industrial Applications
Medical Appliances
Medical/Healthcare Applications
Oil/Gas Applications
Pump Parts
Seals
Surgical Instruments
Users viewing this material also viewed the following: