Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 158 °C | 316 °F | |
Noltex Soarnol® H4815 Ethylene Vinyl Alcohol Copolymer Special designed the highest ethylene content grade. Ethylene content 48 mol%.Information provided by Soarus, LLC. In the United States SOARNOL is produced by Noltex, L.L.C., an affiliate of Nippo.. |
|||
Melting Point | 158 - 166 °C | 316 - 331 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 5130 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 5130 PVDF has an ultra high viscosity ideal for its usage in lithium batteries.Additional Information: Intrinsic Viscosity: 0.27 - 0.37 l/gInformation provided by Solvay Specialty Polymers. |
|||
Melting Point | 158 °C | 316 °F | DSC |
EVALCA EVAL® G156A Ethylene Vinyl Alcohol Copolymer Resin
(discontinued **) 48 mol % Ethylene.Data provided by EVALCA. Applications: Cast film, specialty applications. EVOH is used in packaging applications because of its outstanding gas barrier properties.EVAL™ is now p.. |
|||
Melting Point | 158 - 221 °C | 316 - 430 °F | 0.025" extruded film |
Huntsman IROGRAN® A 94 E 4900 TPU-Polyester Introduction: IROGRAN A 94 E 4900 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a spe.. |
|||
Melting Point | 158 °C | 316 °F | DSC |
Solvay Specialty Polymers Ixan® PVS 119 Polyvinylidene Chloride (PVDC) Ixan® PVS 119 is a PVDC-based blend for extrusion and coextrusion of barrier films for food packaging and medical films. It is recommended for applications that require a very good oxygen and wat.. |
|||
Melting Point | 158 - 168 °C | 316 - 334 °F | ASTM D3418 |
Shanghai Ofluorine D-1 PVDF Lithium Ion Battery Binders (DF-2) Description: D-1 PVDF Powder has good solubility in some solvent, it is more suitable for lithium ion battery industry as binder. D-1 PVDF is a homopolymer with high dielectric constant, which shows.. |
|||
Melting Point | 158 - 162 °C | 316 - 324 °F | 50% humidity, 23°C; ISO 3146 |
Borealis BA11CF Polypropylene Copolymer BA110CF is a heterophasic copolymer. This grade is suitable for use on chill roll processes. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. .. |
|||
Melting Point | 158 - 162 °C | 316 - 324 °F | DSC; ISO 3146 |
Borealis BB213CF Polypropylene Copolymer BB213CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BB213CF is recommended for food packaging.. |
|||
Melting Point | 158 - 162 °C | 316 - 324 °F | DSC; ISO 3146 |
Borealis BD212CF Polypropylene Copolymer BD212CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BD212CF is designed for food packaging, l.. |
|||
Melting Point | 158 - 162 °C | 316 - 324 °F | DSC; ISO 3146 |
Borealis BD712CF Polypropylene Copolymer BD712CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BD712CF is recommended for food packaging.. |
|||
Melting Point | 158 °C | 316 °F | DSC |
Total PPH 3727W Polypropylene, High Performance Injection Molding Grade Balanced Properties TOTAL Polypropylene 3727W strikes an optimum balance between excellent mechanical properties (tensile, flex and impact) and processability making it a superior molding grade for.. |
|||
Melting Point | 158 °C | 316 °F | DSC |
Total PPH 3727WZ Polypropylene, Injection Molding Grade Fina’s new HIGH PERFORMANCE injection molding gradeBalanced Properties - Fina 3727WZ strikes an optimum balance between excellent mechanical properties (tensile, flex and impact) and processability.. |
|||
Melting Point | <= 158 °C | <= 316 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ FL 00728CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00728CC is an excellent coextrusion partner in extrusion coating, blown and cast film. Good adhesion onto OPP in coextrusion. This grade offers excellent optical, low gel and.. |
|||
Melting Point | <= 158 °C | <= 316 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 00728 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00728 is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation.Availability: Africa & Mid.. |
|||
Melting Point | <= 158 °C | <= 316 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 00728CC Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00728CC is a copolymer of ethylene and vinyl acetate.Processing Conditions: Processing temperatures above 220°C (428°F) may cause resin degradation.Availability: Africa & M.. |
|||
Melting Point | 158 °C | 316 °F | Dow Method (DSC) |
Dow XU 32019.10 Barrier Polymer Excellent oxygen and water vapor barrier Information provided by Dow |
|||
Melting Point | 158 °C | 316 °F | Dow Method (DSC) |
Dow XU 32046.31 Barrier Polymer Excellent oxygen and water vapor barrier Information provided by Dow |
|||
Melting Point | 158 °C | 316 °F | |
Arkema Group Pebax® MV 1074 Polyether Block Amide (PEBA) Typical application: Breathable filmInformation provided by Arkema Group |
|||
Melting Point | 158 °C | 316 °F | ISO 11357 |
Arkema Group Pebax® MV 1074 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MV 1074 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MV 1074 SA 01 is an inherently dissipative polymer and can be dry blended or .. |
|||
Melting Point | 158 °C | 316 °F | 10°C/min |
Arkema Group Pebax® MV 1074 SN 01 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....) Permanent antista.. |
|||
Melting Point | 158 °C | 316 °F | ISO 11357 |
Arkema Group Pebax® MV 1074 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MV 1074 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. MV 1074 SP 01 is an inherently dissipative polymer and can be dry blended or .. |
|||
Melting Point | 158 °C | 316 °F | ISO 11357 |
Arkema Group Pebax® MV 3000 SA 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MV 3000 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on .. |
|||
Melting Point | 158 °C | 316 °F | ISO 11357 |
Arkema Group Pebax® MV 3000 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® MV 3000 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on .. |
|||
Melting Point | 158 °C | 316 °F | ASTM D3418 |
Arkema Group Pebax® MV1074 Polyether Block Amide |
|||
Melting Point | 158 °C | 316 °F | ISO 11357 |
Arkema Group Pebax® MV 1074 SA 01 MED Polyether Block Amide (PEBA) Polyether block amide PEBAX® MV 1074 SA 01 MED is a thermoplastic elastomer made of hydrophilic flexible polyether and rigid polyamide. PEBAX® MV 1074 SA 01 MED is an inherently dissipative polyme.. |
|||
Melting Point | 158 °C | 316 °F | (Dry) |
Arkema Group Pebax® MV 1074 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D breathable (high permeability to H2O vapor,CO2,O2) permanent antistatic grade Applications: breathable films (medical, textile....) Permanent antista.. |
|||
Melting Point | 158 °C | 316 °F | |
AIM 70 Fusible Alloy Uses: punch and die in short run sheet metal forming; external and internal support for bending tubing extrusions; holding jet engine blades for machining and broaching; annealing and nitriding seal.. |
|||
Melting Point | 158 - 162 °C | 316 - 324 °F | ASTM D3418 |
Solvay Specialty Polymers Solef® 11010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Melting Point | 158 - 172 °C | 316 - 342 °F | |
Arkema Group KYNAR® HSV Polyvinylidene Fluoride Powder Characteristics: White, non-hygroscopic powder.Applications: Membrane, Lithium ion battery applicationsInformation provided by Arkema Inc. |
|||
Melting Point | <= 158 °C | <= 316 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ AD 2528EH2 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: AD 2528EH2 is a copolymer of ethylene and vinyl acetate. Availability: Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: YesFree Flowing Agent: Yes Applications:Hot Mel.. |