Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total PPH 3727W Polypropylene, High Performance Injection Molding Grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Total Atofina
Trade Name PPH
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PPH 3727W Polypropylene, High Performance Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Balanced Properties TOTAL Polypropylene 3727W strikes an optimum balance between excellent mechanical properties (tensile, flex and impact) and processability making it a superior molding grade for cap and closure applications.Impact Strength 3727W offers improved impact strengthNucleation TOTAL Polypropylene 3727W is formulated to provide fast cycle time and improve contact clarity in thin wall multi-cavity molds.Recommended Applications. TOTAL Polypropylene 3727W is recommended for large thin wall parts, caps and closures.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.905 g/cc
0.905 g/cc
ASTM D1505
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238, L
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.0 MPa
4790 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Tensile Modulus 1.24 GPa
180 ksi
ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256A
Impact Test 18.0 J

@Thickness 3.17 mm
13.3 ft-lb

@Thickness 0.125 in
Drop Impact; API
Thermal Properties Metric English Comments
Melting Point 158 °C
316 °F
DSC
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648