Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis BD212CF Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Borealis
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis BD212CF Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BD212CF is a heterophasic copolymer. This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: BD212CF is designed for food packaging, lamination films, stationary films, and label film.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.900 - 0.910 g/cc
0.0325 - 0.0329 lb/in³
ISO 1183
Melt Flow 5.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
5.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Elongation at Break 600 - 800 %
600 - 800 %
ISO 527-3
Tensile Modulus 0.450 - 0.550 GPa
65.3 - 79.8 ksi
ISO 527-2
Flexural Modulus 1.00 GPa
145 ksi
50% relative humidity; ISO 178
Dart Drop, Total Energy 28.0 J

@Thickness 0.0500 mm
20.7 ft-lb

@Thickness 0.00197 in
1150N; ISO 7765-2
Film Tensile Strength at Break, MD 35.0 - 55.0 MPa
5080 - 7980 psi
ISO 527-3
Film Tensile Strength at Break, TD 30.0 - 50.0 MPa
4350 - 7250 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 158 - 162 °C
316 - 324 °F
DSC; ISO 3146
Vicat Softening Point 145 °C

@Load 1.02 kg
293 °F

@Load 2.25 lb
ISO 306
Optical Properties Metric English Comments
Haze <= 25 %
<= 25 %
Gloss >= 7.0 %
>= 7.0 %
60° of arc; ASTM D2457
Copyright © lookpolymers.com All Rights Reserved