Thermal Properties Metric English Comments
Melting Point 158 - 166 °C
316 - 331 °F
ASTM D3418
Solvay Specialty Polymers Solef® 5130 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 5130 PVDF has an ultra high viscosity ideal for its usage in lithium batteries.Additional Information: Intrinsic Viscosity: 0.27 - 0.37 l/gInformation provided by Solvay Specialty Polymers.
Melting Point 163 - 166 °C
325 - 331 °F
ASTM D3418
Arkema Group Kynar Flex® 3120 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Melting Point 162 - 166 °C
324 - 331 °F
ISO 3146
Borealis Bormed™ DM55pharm Polypropylene
Bormed™ DM55pharm is a low melt flow rate polypropylene homopolymer intended for extrusion and thermoforming. Its very good organoleptic properties allows this grade to be used with any master bat..
Melting Point 162 - 166 °C
324 - 331 °F
DSC; ISO 3146
Borealis HB600TF Polypropylene
HB600TF is a low melt flow rate polypropylene homopolymer intended for extrusion and thermoforming. Its very good organoleptic properties allows this grade to be used with any master batch without ..
Melting Point 162 - 166 °C
324 - 331 °F
DSC; ISO 3146
Borealis HC600TF Polypropylene
HC600TF is a polypropylene homopolymer intended for thermoformed packaging applications. Its very good organoleptic properties allows this grade to be used with any masterbatch without discoloring ..
Melting Point 162 - 166 °C
324 - 331 °F
DSC; ISO 3146
Borealis HD204CF Polypropylene
HD204CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD204CF is recommended for medical applications, inner layer in co extru..
Melting Point 162 - 166 °C
324 - 331 °F
DSC; ISO 3146
Borealis HD234CF Polypropylene
HD234CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD234CF is recommended for food packaging, lamination films, stationery f..
Melting Point 162 - 166 °C
324 - 331 °F
DSC; ISO 3146
Borealis HD244CF Polypropylene
HD244CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: food packaging, lamination films, stationery folders, multi layer co-extr..
Melting Point 162 - 166 °C
324 - 331 °F
DSC; ISO 3146
Borealis HD601CF Polypropylene
HD601CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: metallisable cast film, inner layer in co extrusion, textile packaging fil..
Melting Point 162 - 166 °C
324 - 331 °F
DSC; ISO 3146
Borealis HD621CF Polypropylene
HD621CF is a polypropylene homopolymer This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: food packaging, lamination films, statio..
Melting Point 162 - 166 °C
324 - 331 °F
DSC; ISO 3146
Borealis HD214CF Polypropylene Homopolymer
HD214CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: food packaging, lamination films, stationary films, multi layer co-extrus..