Arkema Group Pebax® MV 3000 SP 01 Polyether Block Amide (PEBA)

Category Polymer , Thermoplastic , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Pebax® MV 3000 SP 01 Polyether Block Amide (PEBA).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyether block amide PEBAX® MV 3000 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This hydrophilic grade when extruded into either a thin film or laminated on to a substrate offers excellent permeability to moisture vapor while remaining waterproof and offering an excellent barrier layer to bacteria. This SP grade is specifically designed for outdoor application that needs excellent weather resistance properties.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
ISO 1183
Water Absorption 28 %

@Temperature 23.0 °C,
Time 86400 sec
28 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Moisture Absorption at Equilibrium 1.0 %

@Temperature 20.0 °C
1.0 %

@Temperature 68.0 °F
50% RH; ISO 62
Water Vapor Transmission 3100 - 4000 g/m²/day

@Thickness 0.0150 mm,
Temperature 38.0 °C
200 - 258 g/100 in²/day

@Thickness 0.000591 in,
Temperature 100 °F
90% RH; ASTM E96 E
19000 - 25000 g/m²/day

@Thickness 0.0150 mm,
Temperature 38.0 °C
1220 - 1610 g/100 in²/day

@Thickness 0.000591 in,
Temperature 100 °F
50% RH; ASTM E96 BW
Mechanical Properties Metric English Comments
Hardness, Shore D 35
35
Instantaneous, Conditioned 15 days at 23°C - 50% RH; ISO 868
Tensile Strength at Break 35.0 MPa
5080 psi
Conditioned 15 days at 23°C - 50% RH; ASTM D638
Elongation at Break 500 %
500 %
Conditioned 15 days at 23°C - 50% RH; ASTM D638
Flexural Modulus 0.0450 GPa
6.53 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Thermal Properties Metric English Comments
Melting Point 158 °C
316 °F
ISO 11357
Processing Properties Metric English Comments
Nozzle Temperature 190 - 210 °C
374 - 410 °F
Blown Film
240 - 250 °C
464 - 482 °F
Cast Film
240 - 250 °C
464 - 482 °F
Coating
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Dry Time 4.00 - 8.00 hour
4.00 - 8.00 hour